The old mounting stem had corrosion that ran through the piece, right to the front. I drilled out the old stem, larger to fit in a replacement, which I turned on a lathe.
At this point, I've blasted, drilled and ground the pits. Then it was striked with copper, and soldered. I ran the bead around the hole for when I put the replacement stem in place.