1863 Remington 31 Caliber (5-Shot) Pocket Pistol loading lever detail. These pieces were dissasembled, sanded and buffed, double copper plated, hand buffed again, and double Nickel Plated. They were hand buffed to a patina finish, not machine buffed to a high gloss mirror finish. All plating, on all pieces was done with the Caswell Plug N Plate systems, none were tank plated. (Clening and de-greasing were done in a heated 2-1/2 Gallon tank, but the plating was all done with the Plug N Plate pen plating wands.