Old 08-01-2003, 03:04 PM
Newbie
 
Join Date: Jun 2003
Posts: 20
tgoode
Default First projects

Here are my first and second completed plating projects!




These are Airsoft guns, not real guns. Basically they are BB guns that run off of compressed gas. They shoot 6mm plastic BBs at 300 feet per second and are used in a sport that is similar to paintball with more of an emphasis on military and tactical simulation.

The slides for both guns are made of 6061 Aluminum. the lower frame of the Springfield is cast aluminum, while the SVI Infinity's frame is pot metal. All of the other small parts such as triggers, sights, safeties, etc are also Pot Metal..

Pot metal parts were primed using the old pot metal primer kit. Everything was finish plated using the standard acidic electroless nickel kit.

I've found that bath temperature is the key to successful pot metal plating. It will prime at lower temperatures, but the best adhesion is at 180 degrees F.

High-res pics are here
Reply With Quote
  #2 (permalink)  
Old 08-03-2003, 03:02 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,376
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

Very nice - can we post them in our Customer Gallery?
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
  #3 (permalink)  
Old 08-03-2003, 07:42 PM
Newbie
 
Join Date: Jun 2003
Posts: 20
tgoode
Default

By all means, you may do that.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Visually Curing projects ? garykelly Powder Coating Questions 2 07-27-2004 01:53 PM


All times are GMT -4. The time now is 03:08 AM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.