Default Holley Carb plating

There are a lot of us out there trying to restore Holley carburetors to their original finish. I am using the Copy Cad kit. I am glass beading the fuel bowls and main body. I then plate with the zinc. It looks pretty good at this point (maybe a little shiny). When I dip into the yellow chromate solution, my parts look way to yellow and shiny. They look just like the steel parts that I have plated. I am wanting the flat "golden" color that these carbs were originally. Should I be using the olive drab dichromate solution? Any help will be greatly appreciated.
Reply With Quote
  #2 (permalink)  
Old 02-10-2004, 04:13 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,360
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

Sounds like you have too much brightener in the Copy Cad. It needs to plate dull.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
  #3 (permalink)  
Old 08-11-2007, 01:08 PM
Amateur Metal Finisher
 
Join Date: Aug 2006
Posts: 140
MrPontiac is on a distinguished road
Default Re: Holley Carb plating

Mach, ive read that as soon as you put the yellow on imediately redip you carb. into a 5% with muratic acid and distilled water for about 10 secands and then redip into distilled water bath. Im getting ready to try it on a Rochester carb. stay tuned ill let you know how it comes out.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Holley Carb. plating 68goat Plating Pot Metal 30 07-24-2007 10:28 PM
Gold Plating and Nickel plating tzmandevil Electroplating Questions 2 09-16-2005 09:11 AM
Nickel bath inexplicably quits plating jackf Electroplating Questions 5 01-25-2005 09:55 PM
A couple carb plating questions KenL Plating Pot Metal 0 01-23-2004 08:34 PM
plating and size power? chromo Electroplating Questions 7 01-18-2003 02:52 AM


All times are GMT -4. The time now is 12:53 AM.


Powered by vBulletin® Version 3.7.0
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.