Plating Pot Metal Plating this troublesome metal can be very challenging. If you have questions, tips or tricks about plating onto pot metal (zinc diecast), this is the place to post them.

Closed Thread
 
LinkBack Thread Tools Display Modes
  #1 (permalink)  
Old 12-19-2004, 02:33 PM
Newbie
 
Join Date: Dec 2004
Posts: 2
taorama
Default Plating Guitar Tremolo w/ Smoked Chrome (newbie)

First time poster here, so forgive my naïve-ness. I've got a number of old Ibanez tremolos that are plated with what they call "Cozmo Black", which is a smoked chrome finish. Several of the pieces have heavy pitting in the finish. I visited with a local plating company here about refinishing them, and the cost was less than half of what it would have been to buy new pieces. Sounded good to me, but then the company promptly went out of business. Fortunately, I was able to get my parts back!

Anyway, the guy I talked to said that these pieces were pot metal, and the pitting was a result of something in the pot metal reacting with the plating (that's what I remember - it was more technical coming out of his mouth...). So, after looking at this site and a number of the posts here, this looks like something that I might be able to do myself.

Here's a pic of one of the base plates:



The textured finish in the middle (where all the holes are) is normal. It's the pitting on the polished surfaces that's the problem.

Just so I'm clear as to the process, what do you think I would need to do this? I've got a sandblasting cabinet I can use to strip the old finish. I don't have a polishing setup, but I could get one easy enough. Which plating kit would be best for my purposes? These are NOT large parts (4"x3"x1"), so I don't need anything huge. I'm pretty clear on the preparation/cleaning stages, but to get the smoked chrome finish, what are the best steps to follow?

Thanks for any help you can provide!

Andy
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #2 (permalink)  
Old 09-07-2005, 09:12 AM
jimcarry's Avatar
Experienced Metal Finisher
 
Join Date: Jul 2004
Location: Arkansas
Posts: 370
jimcarry is on a distinguished road
Send a message via Yahoo to jimcarry
Default Re: Plating Guitar Tremolo w/ Smoked Chrome (newbie)

http://www.caswellplating.com/pickakit
go to this link for the help you are looking for
__________________
Jim Eaton
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
Closed Thread

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


Similar Threads
Thread Thread Starter Forum Replies Last Post
copy chrome vs triple chrome plating splbnd27 Electroplating Questions 18 06-21-2006 08:35 AM
Plating Problem grey finish from chrome plating tshirah Electroplating Questions 2 08-13-2005 01:08 AM
Chrome plating guitar tuner johno697 Electroplating Questions 3 03-29-2005 11:38 PM
NEWBIE Chrome Plating Question???? suparida Electroplating Questions 2 06-26-2002 05:10 PM
Repairing rusted chrome plating Angel Electroplating Questions 2 04-19-2002 11:13 AM


All times are GMT -4. The time now is 12:05 PM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2009, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.3.0
Copyright © Caswell Inc.