  #1 (permalink)  
Old 03-16-2006, 02:13 PM
Newbie
 
Join Date: Mar 2006
Posts: 14
rodman13 is on a distinguished road
Default cast alumn haze

Hello every one I just found this forum and it looks awsome. My name is Bill and I have been polishing for about a year now. I still get in a few binds now and then. This is an art. I did have one question, I know all alumn. is different, but my cast alumn. is my most inconsistant. Some mirror and some will have a gray haze. It's not the compound haze or pits but a casting haze. Its like looking at a dirty mirror. I will re sand and you will see the holes. sand them by hand and more will come out. Any suggestion. Thanx in advance. Bill
Reply With Quote
  #2 (permalink)  
Old 03-16-2006, 02:20 PM
fly fly is offline
Amateur Metal Finisher
 
Join Date: Jun 2005
Location: beaumont misssissippi
Posts: 310
fly will become famous soon enoughfly will become famous soon enough
Default Re: cast alumn haze

After you get to the final step of polishing try the flannel cotton and the blue compound.
__________________
www.chrome-plater.blogspot.com
Reply With Quote
  #3 (permalink)  
Old 03-16-2006, 02:23 PM
pickleboy's Avatar
Metal Finishing Guru
 
Join Date: Feb 2005
Location: belleville michigan
Posts: 635
pickleboy is just really nicepickleboy is just really nicepickleboy is just really nicepickleboy is just really nice
Default Re: cast alumn haze

i think you are talking about the same thing as this other thread. check it out and see.
What the heck?
__________________
when in doubt polish it out/ why replace it when you can refinish it
G2 Polishing and Powdercoating
Reply With Quote
  #4 (permalink)  
Old 03-16-2006, 02:55 PM
Newbie
 
Join Date: Mar 2006
Posts: 14
rodman13 is on a distinguished road
Default Re: cast alumn haze

Well I read that thread from the sound It sounds great. I gave a pm to him for explanation. If you know something about it pickle, I would very much appreciate a pm from you, to see your take on it.
Reply With Quote
  #5 (permalink)  
Old 03-16-2006, 04:08 PM
Newbie
 
Join Date: Mar 2006
Posts: 14
rodman13 is on a distinguished road
Default Re: cast alumn haze

I also always used white never tryed blue. What is it called, and is it better
Reply With Quote
  #6 (permalink)  
Old 03-16-2006, 05:12 PM
fly fly is offline
Amateur Metal Finisher
 
Join Date: Jun 2005
Location: beaumont misssissippi
Posts: 310
fly will become famous soon enoughfly will become famous soon enough
Default Re: cast alumn haze

http://www.caswellplating.com/buffs/buffing.htm
This is the blue compound it works good...
__________________
www.chrome-plater.blogspot.com
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Problems w/ cast aluminum sthomag Metal Polishing Questions 2 02-03-2006 01:41 AM
Problems with cast alum sswee Anodizing Questions 5 07-13-2005 06:13 PM
anodizing cast aluminum 8knots Anodizing Questions 2 06-05-2003 08:27 AM
Cast iron prep ewmorritt Metal Polishing Questions 1 05-28-2003 12:31 AM
Chrome Plating Plastics and Die Cast Metals? nunnc Electroplating Questions 1 05-21-2002 02:45 PM


All times are GMT -4. The time now is 11:38 PM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.