Copy Cad system, Im always reading and trying to figure out certain problems but i see no talk of this. Im getting to much foaming action , its to the point i cannot see my parts while they are being plated, Im relying on my watch and seeing results. Is there a anti foaming ingred. i can use to stop this problem from happening?? Most of my parts are coming out perfect with 2.6 amps and 1.2 volts. HELP!!!
|
![]() |