Plating Pot Metal Plating this troublesome metal can be very challenging. If you have questions, tips or tricks about plating onto pot metal (zinc diecast), this is the place to post them.

Reply
 
Thread Tools Display Modes
  #1 (permalink)  
Old 03-02-2003, 08:35 PM
Newbie
 
Join Date: Feb 2003
Posts: 3
Laird
Default pot metal

Okay, another question. The part I need help with is nickel plated pot metal. I would like to "freshen up" the plating but some of the nickel is gone in places. What do I need to do here ? What do I need to buy? I was thinking plug N plate but now I don't know.

Thanks,
Laird
Reply With Quote
  #2 (permalink)  
Old 03-03-2003, 09:34 AM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,367
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

Is the pot metal showing through anywhere? The best thing to do would be to re-plate the entire part with Flash Copper, then nickel plate.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
PLATING POT METAL............... 48Buick Plating Pot Metal 31 08-29-2007 11:40 AM
Plating over cold metal casting jh2ohouse Electroplating Questions 2 12-16-2006 08:28 PM
Plating pot metal for corrosion protection before painting rspencer Plating Pot Metal 2 08-02-2004 11:39 PM
Refinishing Metal Golf Club Heads BillSchultz Other Metal Finishing Questions 0 08-17-2003 10:40 AM
Pot Metal Plating questions Dave Electroplating Questions 1 04-03-2002 05:37 PM


All times are GMT -4. The time now is 10:45 PM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.