ss-truck
Default Re: Holley Carb. plating

I am new to this , but with all the dipping and coating is there any chance I can plug or paritially plug an air bleed or orfice in the carb . I have spent many hours custom building this carb and don't want to take a chance of ruining it by restricting a passage . help
Thanks
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Holley Carb plating scjmach Plating Pot Metal 2 08-11-2007 01:08 PM
Gold Plating and Nickel plating tzmandevil Electroplating Questions 2 09-16-2005 09:11 AM
Nickel bath inexplicably quits plating jackf Electroplating Questions 5 01-25-2005 09:55 PM
A couple carb plating questions KenL Plating Pot Metal 0 01-23-2004 08:34 PM
plating and size power? chromo Electroplating Questions 7 01-18-2003 02:52 AM


All times are GMT -4. The time now is 12:10 AM.


Powered by vBulletin® Version 3.7.0
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.