Plating Pot Metal Plating this troublesome metal can be very challenging. If you have questions, tips or tricks about plating onto pot metal (zinc diecast), this is the place to post them.

Reply
 
Thread Tools Display Modes
  #1 (permalink)  
Old 08-18-2008, 02:16 PM
Newbie
 
Join Date: Aug 2008
Posts: 2
peterd22 is on a distinguished road
Default need pot metal lamp plated w/copper

Hey guys,
I was wondering if there's anyone from Wyoming/Colorado that can do a small job for me. I have an antique lamp base made out of pot metal. It has a repair of solder at the joint and has some of the original copper plate left on it. I already sandblasted it down to the bare copper and some of the pot metal is showing. The cost of buying the equipment is a little excessive and the local people aren't very helpful. I'd like to have it copper plated, so I can restore the original patina. It's a very old and rare base, so it has to be done by someone very knowledgeable. I don't want to have someone experimenting on the base. The size of it is 22" tall, but only about 2" wide. The base is about 10" across. If you can help, please let me know. Thanks.

-Dave
Reply With Quote
  #2 (permalink)  
Old 08-21-2008, 04:47 AM
Amateur Metal Finisher
 
Join Date: Jun 2006
Posts: 129
tbreaden is on a distinguished road
Default Re: need pot metal lamp plated w/copper

I can do it. Can you send me a picture. Thanks.Todd
Reply With Quote
  #3 (permalink)  
Old 09-02-2008, 12:53 AM
Newbie
 
Join Date: Aug 2008
Posts: 2
peterd22 is on a distinguished road
Default Re: need pot metal lamp plated w/copper

Todd, did you get my email with the picture?
Reply With Quote
  #4 (permalink)  
Old 09-02-2008, 03:45 AM
Amateur Metal Finisher
 
Join Date: Jun 2006
Posts: 129
tbreaden is on a distinguished road
Default Re: need pot metal lamp plated w/copper

Yes I did. I e-mailed you with a quote and my phone #. Please call if you have any questions. Thanks, Todd
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Copper plated ripples carts69 Electroplating Questions 4 06-04-2008 03:44 PM
Need pot metal plated monte Services Offered/Wanted 2 12-03-2006 11:05 AM
Gun Metal Blueing Copper plbetsch Electroplating Questions 1 03-06-2005 01:21 AM
Copper objects to be plated coppersmith Electroplating Questions 1 09-01-2003 09:44 PM
matt black finish on copper-plated steel typewritermuseum Other Metal Finishing Questions 2 03-31-2003 12:47 PM


All times are GMT -4. The time now is 10:09 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.