Hey guys just getting started and have some questions
So far I have a harbor freight gun Modfied to use a cup off the gun and that works great
Got a new 5 hp 19cfm at 90 eaton compressor and ref air dryer
Got the plans for the pa blaster to convert my harbor freight pressure blaster for use in my 5x4x5 blasting cabinet
mostly plan on doing wheels and anything else I can fit in my oven
Running into a issue with media cost and what size grit to run
Northern tool has amberblast for 10 bucks a bag but Im not sure what grit to run for paint removal and giving my parts a decent tooth for the powder
amy help with what kind of media to run and if that amberblast is worth my time
so far i have done a few air cleaner lids and some brackets for my nova just using a wire cup brush a drill and harbor freight powder
stuff turned out good before gun mods and great after
Thanks a bunch
Josh