Well i have! remember ur PC just the outside, not the internals, the engine cools itself with the water running trough it not with the heat exiting the metal itself by the block. I did a rotary 13b and its pulling over 500 whp torbocharged and still no temp issues (and i live in Puerto Rico with an ave temp of 90 deg F)
the engine PC'ed