    I am totally new to powder coating. I am starting a motorcycle project this winter, doing an old school Clubman out of a Honda CB 450. The wheels are spoked with chrome rims and I thought of doing them all black. Is it possible to PC them while they are assembled or do I have to do all seperately. I've seen some done but not sure of the method.
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  2. #2
    Join Date
    Nov 2005
    Posts
    945

    Default Re: Spoked Wheel Questions

    yes, you can coat it with the spokes in place. might want to take it to a shop and make sure they're true first, bc they won't be real adjustable after that.
    Len
    Figure Finishing
    www.FigureEngineering.com
    866-900-4949
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  3. #3

    Default Re: Spoked Wheel Questions

    Thanks for the reply. I am curious as to the best way to support the wheel while coating it. I would assume some sort of axle would be the best as I will have to place it horizontally in an oven to cure.
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  4. #4

    Default Re: Spoked Wheel Questions

    i would take them apart. if you dont, your gonna have a hard time if you ever have to true them up again. take a picture of them before you take them apart. i did a search on lacing spoke wheels and its much easier then you would think. i can lace a wheel in about 5 min. but it does take a while to true them up.
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

+ Reply to Thread

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

     

Similar Threads

  1. Aluminum Wheel Polishing Supply questions
    By sirhc76 in forum Metal Polishing Questions
    Replies: 0
    Last Post: 06-08-2009, 06:47 PM
  2. Some wheel coating questions...pic of my problems inside...
    By Mark_H in forum Powder Coating Questions
    Replies: 5
    Last Post: 12-09-2007, 11:51 AM
  3. Replies: 4
    Last Post: 04-03-2007, 07:29 AM
  4. Alloy wheel polishing questions
    By db_abz in forum Metal Polishing Questions
    Replies: 5
    Last Post: 08-24-2006, 03:31 AM
  5. New guy with some easy questions on wheel job
    By brownnugen in forum Metal Polishing Questions
    Replies: 3
    Last Post: 07-26-2006, 09:24 PM

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts

Search Engine Friendly URLs by vBSEO 3.5.0 RC1 PL1