Thread: should I get a gas BBQ grill for outgas?

  1. should I get a gas BBQ grill for outgas?

    I am thinking I don't want to use my "dedicated" PC oven for outgasing because I think maybe the fumes make the oven very dirty.

    A propane gas grill will get up to 500 in a few minutes and possibly even hotter to outgas those aluminum valve cover and intake manifolds. I don't need the precise temperature control for outgas process anyway. Is it a good idea if I can find one for cheap/free?
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  2. Join Date
    Jul 2008
    Location
    Garland, TEXAS
    Posts
    633

    Re: should I get a gas BBQ grill for outgas?

    Quote Originally Posted by PoorOwner View Post
    I am thinking I don't want to use my "dedicated" PC oven for outgasing because I think maybe the fumes make the oven very dirty.

    A propane gas grill will get up to 500 in a few minutes and possibly even hotter to outgas those aluminum valve cover and intake manifolds. I don't need the precise temperature control for outgas process anyway. Is it a good idea if I can find one for cheap/free?
    Make sure your oven has a vent for smoke and excess pressure relief.... and after outgassing,... wash it down real quick.... It's really no big deal to clean it once in a while,.... Shouldn't take much more than a bit of simple green and a rinse....


    See photos of my work at the following link
    http://s244.photobucket.com/albums/gg6/terrellster/
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  3. Join Date
    Nov 2005
    Posts
    945

    Re: should I get a gas BBQ grill for outgas?

    if you've got so much junk burning off that it's making your oven dirty, degrease it better prior to bake. outgassing does not replace cleaning.
    Len
    Figure Finishing
    www.FigureEngineering.com
    866-900-4949
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

+ Reply to Thread

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

     

Similar Threads

  1. outgas horseshoes
    By ottoplex in forum Powder Coating Questions
    Replies: 1
    Last Post: 10-06-2008, 08:56 PM
  2. Outgas question
    By Crimson in forum Powder Coating Questions
    Replies: 2
    Last Post: 03-26-2006, 09:12 PM
  3. Tricks to minimize outgas?
    By tomg552001 in forum Powder Coating Questions
    Replies: 19
    Last Post: 01-07-2004, 09:15 AM
  4. OUTGAS???
    By tangnut in forum Powder Coating Questions
    Replies: 1
    Last Post: 09-21-2003, 12:27 PM
  5. Outgas Signs
    By 04sp500 in forum Powder Coating Questions
    Replies: 2
    Last Post: 08-02-2003, 01:04 AM

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts

Search Engine Friendly URLs by vBSEO 3.5.0 RC1 PL1