    I have a exhaust set off a motorcylce that needs to be powder coated in high temp black just the end tips. Is the chrome surface a good enough surface to adhere the powder to or does it need to be stripped? Or can it be scuffed up to powder? Any suggestions would be apperciated.

    Thanks

  2. #2
    boston_jake01 is offline Amateur Metal Finisher
    Join Date
    Oct 2006
    Posts
    56

    Default Re: Powder Coating Chrome Question

    as long as the chrome is not peeling or in bad shape you can powder over it and scuffing it is fine.

  3. #3
    luv2fly is offline Newbie
    Join Date
    Feb 2010
    Location
    Auburn, IN
    Posts
    18

    Default Re: Powder Coating Chrome Question

    What happens if it is peeling? What then?

  4. #4
    RFLIVES is offline Newbie
    Join Date
    Nov 2009
    Posts
    7

    Default Re: Powder Coating Chrome Question

    Blast it or sand it down to bare metal the coating is only as good as the substrate it's on.

  5. #5
    luv2fly is offline Newbie
    Join Date
    Feb 2010
    Location
    Auburn, IN
    Posts
    18

    Default Re: Powder Coating Chrome Question

    Quote Originally Posted by RFLIVES View Post
    Blast it or sand it down to bare metal the coating is only as good as the substrate it's on.
    Some time ago I was told on another forum that if chrome had begun peeling, etc., that for best results the nickel and copper had to be removed prior to PC otherwise the corrosion would resurface under the PC? Didn't quite make sense to me if no oxygen could penetratet the PC, the the part shold otherwise act as normal.

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

Similar Threads

  1. powder coating question...
    By robert_t_wallace in forum Oven Building Forum
    Replies: 13
    Last Post: 08-18-2009, 07:20 AM
  2. Powder coating intake question
    By ng8264723 in forum Powder Coating Questions
    Replies: 1
    Last Post: 02-21-2009, 10:08 AM
  3. Powder Coating Booth Question??
    By welterracer in forum Powder Coating Questions
    Replies: 4
    Last Post: 06-06-2008, 09:16 AM
  4. Powder Coating Question
    By ptim in forum Powder Coating Questions
    Replies: 4
    Last Post: 02-27-2007, 11:10 PM
  5. Powder Coating (Chrome) Question...
    By TCalYen in forum Powder Coating Questions
    Replies: 3
    Last Post: 05-12-2004, 11:24 AM

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •