    wondering if it's possible or if anyone has done it. i've seen some paints that claim to stand up to 1200 degrees.

    seems like it may work and might be ideal for some custom artwork with a clear powder coat. later.

  2. #2
    baz
    baz is offline Metal Finishing Guru
    Join Date
    Feb 2006
    Posts
    822

    Default Re: powder coating over high temp paint.

    high heat paints usually contain silicone so anything on top of it will have adherence problems. even if the powder would stick to the high heat paint any clear would turn yellow in no time.

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

Similar Threads

  1. High temp coating for headers?
    By jaysouth2000 in forum Powder Coating Questions
    Replies: 4
    Last Post: 05-15-2008, 07:19 PM
  2. High temp Powder coating Problems
    By smackgod in forum Powder Coating Questions
    Replies: 12
    Last Post: 03-22-2008, 08:56 AM
  3. High Gloss paint to match powder?
    By DriKote in forum Powder Coating Questions
    Replies: 1
    Last Post: 05-19-2006, 09:09 PM
  4. Can I use VHT high Temp with Krylon High temp radiator paint
    By magnus in forum Other Metal Finishing Questions
    Replies: 1
    Last Post: 05-03-2003, 11:20 AM

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •