    Default Powder Coating 2 diff, colors????

    I am wondering how to powder coat with 2 deff colors. For example i see alot of intakes or valve colors that are one color and the "raised" letters are another color. How is that done?

  2. #2
    XaboveX112's Avatar
    XaboveX112 is offline Newbie
    Join Date
    Mar 2009
    Location
    Cicero, NY
    Posts
    45

    Default Re: Powder Coating 2 diff, colors????

    It depends on what you are trying to accomplish and there are many differnt ways to do it... One way to do it is to spray your base coat (in this case lets say you want the raised letters white and the cover blue) of white, Fully cure your white base coat then once cool tape off your raised letters and spray your blue.... At this point you can carefully pull off your tape and then put in the oven to cure your blue.... Or you can spray your white like before and when you spray your blue powder use a damp towel or q-tip and remove the blue poweder that way... Definatly takes some practice but its definatly do able... Good luck to you

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

Similar Threads

  1. accidently got diff color powder on hot part
    By motoman3b in forum Powder Coating Questions
    Replies: 6
    Last Post: 06-12-2009, 06:48 AM
  2. Problems with coating candy colors!Need HELP!
    By pcp5578 in forum Powder Coating Questions
    Replies: 2
    Last Post: 04-03-2009, 09:52 PM
  3. Powder coating wheels... two colors? General advice.
    By UrineMachine in forum Powder Coating Questions
    Replies: 9
    Last Post: 04-14-2007, 11:20 AM
  4. diff in powder coating guns
    By boucher in forum Powder Coating Questions
    Replies: 2
    Last Post: 05-05-2004, 08:23 PM
  5. 19 New Powder Colors
    By mcaswell in forum Powder Coating Questions
    Replies: 0
    Last Post: 03-29-2003, 10:51 PM

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •