I'm powder coating jewelry and next on my list is a metal neckwire. To be worn the neckwire must be bent ever so slightly to fasten it. I tried coating wire once just to see if I could bend it and the coating cracked. Granted a neckwire will not actually be bent, only submitted to slight pressure, but I need to find a coating that can handle it. Anyone know of such a coating or brand of coating Thanks everyone, you're always so helpful. A. Derenthal Cry Baby Designs |
|
|||
|
Technically speaking....all fluoropolymer coatings are malleable to a certain extent. You didn't say what your substrate was, nor if you were the applicator of the coating. I'd assume that if ferrous or even non-ferrous substrate, and it needed to lay against the skin (acidic environment) that your application would need something micro-thin just to protect the user? I may be totally off base here, but I'm thinking something along the lines of Parylene ( measured down to the micron, not mil) or something of that sort. but then again...you didn't state as to you wanted to replicate "gold" or not either. Just a wee bit more info if you can would be helpful in solving your conundrum. Thanks
|
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Powder coating on firearms | LoneGunman | Powder Coating Questions | 2 | 06-15-2006 01:54 PM |
| Removal of unknown coating on aluminum | rclint | Metal Polishing Questions | 6 | 08-25-2005 01:04 AM |
| Coating Brake Rotors | rickanderson53 | Other Metal Finishing Questions | 4 | 08-19-2005 12:15 AM |
| A few coating questions | PhilipK | Powder Coating Questions | 10 | 12-22-2004 12:38 AM |
| Non-paint powder coating | dshepherd | Powder Coating Questions | 6 | 01-26-2004 12:49 PM |