Quote:
Originally Posted by drfjr1976
Here is what I use on every part that I coat.


*website edited by non-stick*

ehhhhhh..... this is where I have to look like the bad guy. I seriously wish I didn't have to bud,honest. Let's give it a little more time before we go that route and see if something from a Home-Depot or Lowes type of site can't be found,k? Sorry.... It's not often I have to put the moderator hat on, but I hope you understand the position it puts me in. With the talent in this forum, I'm sure a reasonable solution can be had.
Reply With Quote
  #22 (permalink)  
Old 01-11-2004, 10:54 PM
customandsound
Guest
 
Posts: n/a
Default

i was told that for small parts like waternecks little brackets that a toaster oven would work for that ... but i don't know .. i only polish metal.. but i am looking in to learing the powder coating trade ...
Reply With Quote
  #23 (permalink)  
Old 01-11-2004, 11:32 PM
Amateur Metal Finisher
 
Join Date: Aug 2003
Posts: 97
duke
Default

that is the best price i've seen. specially with no freight cost.
cheers
Reply With Quote
  #24 (permalink)  
Old 01-13-2004, 01:47 PM
Newbie
 
Join Date: Jan 2004
Posts: 17
BRANDONPEAKE
Default

im looking into buying one and ive got to get it somewhere and id rather buy it from here so i can get most of the stuff from the same place
Reply With Quote
  #25 (permalink)  
Old 05-19-2005, 11:35 PM
Experienced Metal Finisher
 
Join Date: Apr 2004
Posts: 466
jtagger19 is on a distinguished road
Default

to get to temp it takes about 1 hour
at least that was my experience.
Reply With Quote
  #26 (permalink)  
Old 05-25-2005, 12:43 AM
Amateur Metal Finisher
 
Join Date: Oct 2004
Location: Lake Mary, FL
Posts: 56
jagboy69
Default

DId someone mention RC car parts How about buying a crappy toaster oven from Wally world That would work perfectly for you and not take up much space.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
1500 w lamp suprtong Powder Coating Questions 1 03-12-2005 07:50 PM
Ir Lamp somebody help me!!! Sezer Powder Coating Questions 4 06-11-2004 12:33 AM
polishing a brass lamp artp Metal Polishing Questions 2 02-02-2004 12:13 PM
lamp heat duke Powder Coating Questions 13 01-06-2004 01:44 PM
Lamp Reflector plating Marcos Electroplating Questions 1 02-15-2003 02:37 PM


All times are GMT -4. The time now is 10:13 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.