Amateur Metal Finisher
 
Join Date: May 2003
Posts: 162
Fireblade
Default

I offered to give this a shot, don't know if anyone else has before me, but if they did not we will see. I'll try and do it quickly as I can.
Reply With Quote
  #12 (permalink)  
Old 12-13-2003, 04:23 PM
Amateur Metal Finisher
 
Join Date: Aug 2003
Posts: 97
duke
Default

good on ya mate. can't wait to see the results.

cheers
Reply With Quote
  #13 (permalink)  
Old 01-19-2004, 10:05 PM
customandsound
Guest
 
Posts: n/a
Default

what was the results ?
Reply With Quote
  #14 (permalink)  
Old 01-19-2004, 11:14 PM
Experienced Metal Finisher
 
Join Date: Dec 2002
Location: Central New York
Posts: 353
DALE will become famous soon enough
Default

He still has had a chance to finish the test last time he checked back about it.
Reply With Quote
  #15 (permalink)  
Old 01-20-2004, 01:31 AM
Amateur Metal Finisher
 
Join Date: Mar 2003
Location: S. IL.
Posts: 109
drfjr1976
Default

Is it really that difficult to apply Silvaspray that the average "joe" couldn't do it himself?
Reply With Quote
  #16 (permalink)  
Old 01-20-2004, 11:38 AM
Amateur Metal Finisher
 
Join Date: May 2003
Posts: 162
Fireblade
Default

My cousin is doing it this weekend, and I should have results by mid next week. FINALLY!!!!! lol
Reply With Quote
  #17 (permalink)  
Old 01-20-2004, 12:06 PM
Experienced Metal Finisher
 
Join Date: Sep 2003
Location: CT-NY-NJ area
Posts: 359
non-stick
Default

lol....it's a bear waiting on other people at times,huh? What about that other stuff that Dale recommended? That looked promising as well. I don't know if this is possible or not with the sample that you have, but do you think you can test the silvaspray out on some plastic pieces as well so we know how valid a coating it can be on car related trim items and such? I've been dying to know how that would look as the only pictures to be found on this site are from a dash insert for a mopar B-Body.
Reply With Quote
  #18 (permalink)  
Old 01-20-2004, 05:47 PM
Amateur Metal Finisher
 
Join Date: May 2003
Posts: 162
Fireblade
Default

I will try and find a piece of plastic sometime this week that I can use as well. I am heading to grainger sometime this week, I will pick up a small piece of hi-temp stuff as well.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Ovens with gas question getastro Powder Coating Questions 22 11-08-2004 01:06 PM
Peak voltage question mudwhump Anodizing Questions 6 01-14-2004 11:53 PM
Brand Newbie Aluminum Polishing Question gdsegel Metal Polishing Questions 1 04-25-2003 09:04 AM
Rookie question aermakov@rogers.com Electroplating Questions 1 11-12-2002 04:24 PM
Got a question or 2 Darvil Electroplating Questions 2 05-02-2002 01:10 AM


All times are GMT -4. The time now is 09:09 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.