Default Home Made Powder Booth

I am thinking of using a cardboard box. Its actually a old computer box. I am planning on trying to use a smaller shop vac to suck up the excess powder, but just not sure where to place the hose at. (Towards the top, bottom, or in the middle of the backside of the box? Any ideas would be great and helpful. Oh, and should i use like furnace filters to help catch any of the powder or just let the vacuum do its thing? Where can i get the sifting screens at? I cant seem to find any screen that matches any of the mesh # that were posted some where on this forum.

Thanks Mike
Reply With Quote
  #2 (permalink)  
Old 01-25-2004, 07:56 AM
Experienced Metal Finisher
 
Join Date: Sep 2003
Location: CT-NY-NJ area
Posts: 359
non-stick
Default

cardboard boxes have been used here with great success. I'd place the hole dead center in the back. Whether or not to use a filter is up to you. Some do, some don't. Personally I'd just let it free flow and have the most suction you can have. Try it with a little bit of filter and let us know how it works out please. As for the screens... I have no doubt they are being looked into for the best way in how to be offered for you guys and something will turn up shortly for purchasing options.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Tips and Tricks non-stick Powder Coating Questions 27 11-11-2007 03:01 PM
powder coating over powder coat? corybarta Powder Coating Questions 6 08-21-2006 09:15 AM
Finding a place to powder coat RCLSolutions Powder Coating Questions 3 05-04-2005 10:42 PM
Gun spitting excess powder pdeinc Powder Coating Questions 8 10-21-2004 04:21 PM
Powder Booth on a DIET!!!! Noob2PC Powder Coating Questions 6 04-10-2004 08:51 PM


All times are GMT -4. The time now is 08:37 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.