ok, say i want to put down an 'aluminum' basecoat first, then follow up with a 'candy blue'. should i put the aluminum on first and bake it THEN put the candy blue on? or should i put the aluminum on, then spray the candy blue on THEN bake? thanks. also, about how long should i be letting these items cook? ive been doing 400 degrees for 20 mins... is that too long?
|
|
|||
|
You would want to spray the aluminum and then bake it, and then you would want to spray the candy blue. I am assuming the candy blue is a translucent. The time that you posted sound right to me.
|
|
|||
|
ok, what about putting 2 coats of powder on something? for the most shiny finish, should i use the first coat only? what about gloss... i bought a 2lb thing of gloss, but havent really used it. from what i did, it tends to dull the color (reflective chrome). is it safe to do 2 coats of the same color, then say a clear coat?
|
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| multiple colors | sswee | Powder Coating Questions | 6 | 07-27-2005 08:19 AM |
| when doing multiple PC coats..... | strongtower | Powder Coating Questions | 4 | 05-21-2004 01:44 PM |
| whats the best way to go about two colors on one part? | red99ls1ta | Powder Coating Questions | 2 | 02-24-2004 11:00 PM |
| Problems with clear, flowout, multiple colors, more... | allcarfan | Powder Coating Questions | 3 | 08-25-2003 10:49 PM |
| anodizing with multiple colors | july_favre | Electroplating Questions | 1 | 01-08-2003 06:39 PM |