  #1 (permalink)  
Old 04-07-2004, 05:42 PM
Amateur Metal Finisher
 
Join Date: Jan 2004
Location: Beaufort, SC
Posts: 121
WAORacing
Default Where's the Photo Album?

where is the photo album? Its not up at the top of the page any more.
Reply With Quote
  #2 (permalink)  
Old 04-07-2004, 07:26 PM
Experienced Metal Finisher
 
Join Date: Dec 2002
Location: Central New York
Posts: 353
DALE will become famous soon enough
Default

I was just wondering the same thing
Reply With Quote
  #3 (permalink)  
Old 04-07-2004, 07:50 PM
Noob2PC's Avatar
Experienced Metal Finisher
 
Join Date: Mar 2004
Location: Greensboro NC
Posts: 315
Noob2PC
Default

Non-Stick broke it!
Reply With Quote
  #4 (permalink)  
Old 04-07-2004, 08:26 PM
Blademan's Avatar
Experienced Metal Finisher
 
Join Date: Mar 2004
Location: Gold Beach, Oregon
Posts: 322
Blademan is on a distinguished road
Default

well there went all my aspirations of posting all the fantastic things I've coated.....................LOL......... like my shoes, pants, and wifes car that she's still Bit*** about...hell it's just over spray....is it ?
Reply With Quote
  #5 (permalink)  
Old 04-07-2004, 09:28 PM
customandsound
Guest
 
Posts: n/a
Default

that is a good one ? wonder where it went
Reply With Quote
  #6 (permalink)  
Old 04-08-2004, 08:21 AM
Newbie
 
Join Date: Feb 2004
Location: Syracuse, NY
Posts: 3
Woodfrag
Default

It looks like they upgraded to PHPBB 2.08 and never modded the header files to add the link back.
Reply With Quote
  #7 (permalink)  
Old 04-08-2004, 09:28 PM
Experienced Metal Finisher
 
Join Date: Dec 2002
Location: Central New York
Posts: 353
DALE will become famous soon enough
Default

Quote:
Originally Posted by Woodfrag
It looks like they upgraded to PHPBB 2.08 and never modded the header files to add the link back.
Or the technical explanation ----- OOPS!!!
Reply With Quote
  #8 (permalink)  
Old 04-08-2004, 10:48 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,359
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

Fixed now. If you guys didn't keep ordering stuff, I'd have more time to play with the forum.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
  #9 (permalink)  
Old 04-09-2004, 12:56 AM
Amateur Metal Finisher
 
Join Date: Feb 2004
Posts: 109
dagobert
Default

Quote:
Originally Posted by caswell
Fixed now. If you guys didn't keep ordering stuff, I'd have more time to play with the forum.
Sorry 'bout that, but after reading and posting long enough, at SOME point we gotta get the kits ourselves to be able to share in the fun, right?
Reply With Quote
  #10 (permalink)  
Old 04-10-2004, 08:35 PM
customandsound
Guest
 
Posts: n/a
Default

Quote:
Originally Posted by caswell
Fixed now. If you guys didn't keep ordering stuff, I'd have more time to play with the forum.
ordering i need to find time to place a nice order i am running low on stock ... but monday is right around the corner
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
New photo in the album rides20 Metal Polishing Questions 4 06-11-2005 12:57 AM
Photo album - motorcycle wheel with rainbow flake... powder? mtnbiker Powder Coating Questions 7 04-11-2005 04:28 PM
Silvachrome Photo examples polygon Other Metal Finishing Questions 4 03-25-2003 11:45 PM


All times are GMT -4. The time now is 10:14 AM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.