Default DO NOT blast with play sand

Blasting with play sand generates large amounts of silica dust. The particles can be fine enough to escape most dry dust collectors. Nuicance dust masks do not provide adequate protection from the dust. Only a high level filtration mask will protect you if you insist on blasting with play sand. Here is a link to a fact sheet on the disease called silicosis that is caused by exposure to silica dust. This is important reading for anyone who does a lot of sand or bead blasting. Glass beads may create hazardous dust as well. As coaters, we sometimes have no idea what is contained in the coatings we are trying to blast off the parts to be finished. I would urge everyone to invest in a good filtration(respirator) style mask. This is my opinion. I am not a doctor, just a concerned member of our little micro-community at the Caswell BBS.

http://www.who.int/oeh/OCHweb/OCHweb.../Silicosis.htm
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #2 (permalink)  
Old 04-12-2004, 08:07 PM
customandsound
Guest
 
Posts: n/a
Default

that is true ... it is all right ...
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
Closed Thread

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


Similar Threads
Thread Thread Starter Forum Replies Last Post
sand blasting cabinet...relocated to tips n tricks section duke Powder Coating Questions 15 12-30-2007 12:28 PM
info on blast media Blademan Powder Coating Questions 7 05-18-2007 07:58 PM
Sand Blasting Q? cypress_33415 Other Metal Finishing Questions 3 12-26-2005 09:08 PM
Do you need to sand blast for PC to adhere? Any other ways? krsimulis Powder Coating Questions 4 07-01-2004 09:14 AM
My Space Saver Sand Blast cabinet Noob2PC Powder Coating Questions 6 03-25-2004 09:38 PM


All times are GMT -4. The time now is 07:24 AM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2009, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.3.0
Copyright © Caswell Inc.