newbie to PCing. my first project is the two alloy wheels on my sportbike. the color i like best is (i think) an RAL color called "Hot Red". it is a florescent one and the color chips said something like "two step" or "two coat" or something. is this typical for such colors? i see that Caswell has a selection called "Safety Red" but it's hard to tell if it has that "florescent" quality or not.
anyone out there ever do these "types" of colors,and if so - any tippage? thanks in advance. |
|
|||
|
Just from the color sample panels I have here is some info. I'm still a newbie in PCing as well, but hope this bit of info helps. Yes it is noraml to have to do a 2 coat process for "most" of the fluorescent colors. You have 2 kinds of fluorescent colors the 1 coat process and the 2 coat process. The one coat fluorescent colors don't look near as bright, well I know you can tell big difference in the yellow one and yellow two coat. For the fluorescent 2 coat I believe its always a "white basecoat" then the fluorescent color on top of it.
|
|
|||
|
Nuttyman!
hey, that sounds cool. more questions though: what if you only blasted the aluminum wheel, not "polish up"? do you think that would darken (defract, actually) the brightness of a one-coat neon powder? also, what neon/florescent powders are/were you using and on what, if i amy ask? |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| New Powder Colors, Sizes, and Technical Data | mcaswell | Powder Coating Questions | 13 | 06-21-2007 12:16 PM |
| Flourescent Colors | CaptainChauncy | Powder Coating Questions | 2 | 02-17-2005 05:21 PM |
| Need help..... Looking for Arctic Cat colors | Sleepr_Tech | Powder Coating Questions | 0 | 08-02-2004 07:49 PM |
| Problems with clear, flowout, multiple colors, more... | allcarfan | Powder Coating Questions | 3 | 08-25-2003 09:49 PM |