Anyone know of some hi-temp tape I can use for masking. I got some of the green tape but it tends to curl a little once exposed to the heat. Need something that sticks a little better.
Thanks in advance for the help. |
|
|||
|
I can't say that I have that much trouble with the tape sticking. The only time I have is when it it placed over a hole and the heat builds up pressure inside causing it to blow off, solved this by putting a small hole in the center to relieve the heat. I also apply the tape after pulling the part from the oven after the preheat. This way the part is warm and help the tape stick better, I than go over it with the back end of my hobby nife just to make sure it is all adhered.
|
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| tape | customandsound | Powder Coating Questions | 3 | 06-16-2005 09:41 AM |
| hi temp tape shrinking | craigcraig | Powder Coating Questions | 10 | 11-27-2004 11:04 PM |
| high temp tape | randygrapes218 | Powder Coating Questions | 3 | 07-29-2004 08:57 PM |
| Powder Coating Masking Tape Now Available | mcaswell | Powder Coating Questions | 0 | 08-21-2003 02:13 PM |
| Looking for masking tape recomendations. | chcarver | Metal Polishing Questions | 0 | 03-06-2003 02:51 PM |