Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum  

Go Back   Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum > Powder Coating Questions

Notices

Powder Coating Questions Discussion Board For powder coating questions.

Reply
 
Thread Tools Display Modes
  #1 (permalink)  
Old 06-08-2004, 10:48 AM
Newbie
 
Join Date: Apr 2004
Location: Lenexa, KS
Posts: 22
kcrails
Default First successful powder coating project!

Pics posted before and after. Brake calipers and rotors on Dad's 94 Corvette. The calipers were done using Caswell's PCP56016 Safety Red, and the black centers on the rotors were Caswell's PCP51008 Black Magic. Couldn't have been easier to coat, but took a week of evenings sandblasting the original coating off (epoxy-based caliper paint). Just wanted to say thanks for all the good tips I read on here! Wouldn't have come out half as good without the help.
Reply With Quote
  #2 (permalink)  
Old 06-08-2004, 10:18 PM
Blademan's Avatar
Experienced Metal Finisher
 
Join Date: Mar 2004
Location: Gold Beach, Oregon
Posts: 322
Blademan is on a distinguished road
Default

Looks to me like you did a nice job.....hehehehe I know about them epoxys...you should try a set of valve covers done in the marine epoxy....sandblasters nightmare for sure...
Reply With Quote
  #3 (permalink)  
Old 06-09-2004, 10:58 PM
Bud Bud is offline
Amateur Metal Finisher
 
Join Date: May 2004
Posts: 54
Bud
Default

Wheres the pictures at....? Didn't see any in the album..
Reply With Quote
  #4 (permalink)  
Old 06-10-2004, 02:33 PM
Newbie
 
Join Date: Apr 2004
Location: Lenexa, KS
Posts: 22
kcrails
Default

I just clicked on "Album" at the top of the page, currently they're the first and second pics.. Though the thumbnails look almost black and white, click on them and you'll get the full color versions.
Reply With Quote
  #5 (permalink)  
Old 06-11-2004, 12:47 AM
Bud Bud is offline
Amateur Metal Finisher
 
Join Date: May 2004
Posts: 54
Bud
Default

There they are, they weren't there last night for some reason.
Reply With Quote
  #6 (permalink)  
Old 06-28-2004, 05:07 AM
upncoming's Avatar
Amateur Metal Finisher
 
Join Date: Jun 2004
Location: levittown PA
Posts: 111
upncoming
Send a message via AIM to upncoming Send a message via Yahoo to upncoming
Default Re: First successful powder coating project!

Quote:
Originally Posted by kcrails
Pics posted before and after. Brake calipers and rotors on Dad's 94 Corvette. The calipers were done using Caswell's PCP56016 Safety Red, and the black centers on the rotors were Caswell's PCP51008 Black Magic. Couldn't have been easier to coat, but took a week of evenings sandblasting the original coating off (epoxy-based caliper paint). Just wanted to say thanks for all the good tips I read on here! Wouldn't have come out half as good without the help.

hey did you rebuild them when you did this?
__________________
D.I.L.U.S.I.

Drive It Like You Stole It
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
*** WE ARE GIVING AWAY FREE POWDER COATING *** mcaswell Powder Coating Questions 197 07-08-2008 12:31 PM
powder coating over powder coat? corybarta Powder Coating Questions 6 08-21-2006 08:15 AM
Powder coating on firearms LoneGunman Powder Coating Questions 2 06-15-2006 12:54 PM
My first powder coating project.. Smallblock Powder Coating Questions 1 09-15-2004 08:50 PM
Non-paint powder coating dshepherd Powder Coating Questions 6 01-26-2004 11:49 AM


All times are GMT -4. The time now is 09:05 AM.