If it's mixed with white P/C, I understand it looks a little chalky, and has that greenish watch-hand glow. But what if you mix it with other colors? Does it tint other colors in any certain way? And also, if you mix it with a red, does the red affect the glow color? What about if you shoot it mixed with a white, and then coat that with a translucent candy color? Also, has anyone tried mixing it with metalflake to see if the metal flakes would reflect the glow and sparkle in the dark? I look forward to trying out some of these things, but no sense in reinventing the wheel, especially if the wheel it creates winds up square.
|
|
||||
|
dont get to excited....yet...if you mix it with a clear it seems to work fine..now for the fun part...you can get it in pink,blue (spendy) red and the normal glow..i use it on fishing lures...its tricky....i would suggest not.. NOT mix it in a nother powder other than clearcolor..its like askin for trouble....... if your going for the pre mixed stuff...well i have always been disappointed on anything other than lures..just my trials with glo's over the years
|
|
||||
|
well if anybody is interested in trying this out the link i have for it is~~>http://www.glowpaintpro.com/glow_powder.html...share with us how it comes out if you do it.
__________________
D.I.L.U.S.I. Drive It Like You Stole It |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Tips and Tricks | non-stick | Powder Coating Questions | 27 | 11-11-2007 03:01 PM |
| glow in the dark addtive | mort3 | Powder Coating Questions | 1 | 05-06-2005 10:39 AM |
| Glow in the Dark | PhilM | Powder Coating Questions | 6 | 01-28-2005 03:52 PM |
| Gun spitting excess powder | pdeinc | Powder Coating Questions | 8 | 10-21-2004 04:21 PM |
| Make Your Parts Glow | mcaswell | Powder Coating Questions | 8 | 04-05-2004 07:00 AM |