Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum  

Go Back   Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum > Powder Coating Questions

Notices

Powder Coating Questions Discussion Board For powder coating questions.

FREE POWDER COATING SYSTEM

Until 8/31 - Buy an HV System, Get a Regular PC System FREE! Two systems for the price of one! (Limited Time - US Customers Only)

HV Powder Coating System

Buy Now


Reply
 
Thread Tools Display Modes
  #1 (permalink)  
Old 06-25-2004, 10:19 PM
Amateur Metal Finisher
 
Join Date: Jun 2004
Location: massachusetts
Posts: 63
randygrapes218
Default out gasssing and pre heating?

do you have to pre heat all parts or just certian types of metal? same goes for outgassing is it all type of metal or just the part isnt clean enough? how long do you pre heat for? and do you let the part cool down completely and rewash it with cleaner before shooting? thanks for any info... i am glad i found this site, the prices on alot of the stuff is really good and this message board rocks for us newbies... thanks again to all who reply and help us out and thanks to caswell for having this board...
Reply With Quote
  #2 (permalink)  
Old 06-26-2004, 12:09 AM
Newbie
 
Join Date: Jun 2004
Posts: 12
Kiyi
Default

From my limited experience, the only thing I had to outgas and preheat was aluminum items, Such as valve covers and manifolds.

my first valve cover is at www.kiyi.net
Reply With Quote
  #3 (permalink)  
Old 06-26-2004, 04:54 PM
Experienced Metal Finisher
 
Join Date: Dec 2002
Location: Central New York
Posts: 353
DALE will become famous soon enough
Default

I prebake everything as an extra measure to remove any missed oils.After washing I bake it to dry and then leave in about 5 minutes extra to burn clean. Remove from oven alow to cool until you can hold in hand then coat.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


All times are GMT -4. The time now is 10:20 AM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.