Default Chrome / Candy

I know this has probably been repeatedly covered, but I could use a little clarification. I want to use chrome poly as a base, then top with candy red. What is the exact cure schedule for each and is there anything that needs to be done to the part in between coats? Thanks in advance
Reply With Quote
  #2 (permalink)  
Old 07-01-2004, 07:24 PM
getastro's Avatar
Amateur Metal Finisher
 
Join Date: May 2003
Location: NSB, FL.
Posts: 59
getastro
Default

Cure the chrome for half of the full cure time, let part cool down then spray candy color. Cure at full temp and time. Done
Reply With Quote
  #3 (permalink)  
Old 07-02-2004, 07:28 PM
Newbie
 
Join Date: Jul 2004
Posts: 17
Millermatic
Default

I'll give it a shot, thanks for the info.
Reply With Quote
  #4 (permalink)  
Old 07-03-2004, 07:25 PM
Newbie
 
Join Date: Jul 2004
Posts: 17
Millermatic
Default

It didn't work...for whatever reason, the chrome came out great, it cooled, then when I went to apply to candy, it wouldn't stick to the chrome. Help?
Reply With Quote
  #5 (permalink)  
Old 07-04-2004, 01:10 PM
getastro's Avatar
Amateur Metal Finisher
 
Join Date: May 2003
Location: NSB, FL.
Posts: 59
getastro
Default

If you are using a hobby style gun, try spraying the second coat when the part is warm. this should make the second coat hold. just watch how much you spray, you can over coat the part by doing it this way.
Reply With Quote
  #6 (permalink)  
Old 07-05-2004, 01:12 AM
Amateur Metal Finisher
 
Join Date: Jan 2004
Location: Beaufort, SC
Posts: 121
WAORacing
Default

Quote:
Originally Posted by Millermatic
It didn't work...for whatever reason, the chrome came out great, it cooled, then when I went to apply to candy, it wouldn't stick to the chrome. Help?
Sounds like you didnt have good ground to me. I have had to try several different pieces to get use to shooting the translucents myself. They seem do seem to alittle more difficult to get the right amount applied, so you dont get any bleed through of the chrome or to much build on the corners to where you can see a color difference. Just practice is all i can say.
Reply With Quote
  #7 (permalink)  
Old 07-05-2004, 11:46 AM
Noob2PC's Avatar
Experienced Metal Finisher
 
Join Date: Mar 2004
Location: Greensboro NC
Posts: 315
Noob2PC
Default

I have a piece that I have shot 3 times and still need to shoot it again (don't Ask ). But I have never had any problem with powder sticking on the 2nd or 3rd coat.
Reply With Quote
  #8 (permalink)  
Old 07-28-2004, 01:22 AM
upncoming's Avatar
Amateur Metal Finisher
 
Join Date: Jun 2004
Location: levittown PA
Posts: 111
upncoming
Send a message via AIM to upncoming Send a message via Yahoo to upncoming
Default

Quote:
Originally Posted by Noob2PC
I have a piece that I have shot 3 times and still need to shoot it again (don't Ask ). But I have never had any problem with powder sticking on the 2nd or 3rd coat.
how many times can you PC the same part?
__________________
D.I.L.U.S.I.

Drive It Like You Stole It
Reply With Quote
  #9 (permalink)  
Old 07-28-2004, 08:51 AM
Experienced Metal Finisher
 
Join Date: Dec 2002
Location: Central New York
Posts: 353
DALE will become famous soon enough
Default

For those of you who are having trouble getting the candy/translucent colors to stick switch from chrome to silver. it's a little darker (not much) but coats much easier.
Reply With Quote
  #10 (permalink)  
Old 07-28-2004, 06:07 PM
upncoming's Avatar
Amateur Metal Finisher
 
Join Date: Jun 2004
Location: levittown PA
Posts: 111
upncoming
Send a message via AIM to upncoming Send a message via Yahoo to upncoming
Default

will the translucent look as good as the crome base when you use the silver ?
__________________
D.I.L.U.S.I.

Drive It Like You Stole It
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
copy chrome vs triple chrome plating splbnd27 Electroplating Questions 18 06-21-2006 07:35 AM
Copy Chrome Start-up Elitefisherman Electroplating Questions 10 04-18-2004 04:24 AM
Copy Chrome Questions junodale Electroplating Questions 13 03-17-2004 11:15 AM
Chrome (re)plating question - howto olaf_sc Electroplating Questions 1 07-29-2003 02:00 PM
Hard chrome vs triple chrome butters Electroplating Questions 1 02-19-2003 11:35 PM


All times are GMT -4. The time now is 02:33 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.