I have done spot checks on a lot of the parts I pull out of the oven at 400, given that the parts have been coated the digital laser never comes close to 400 on a standard 20 min dwell time. More time and accurate temp measurements test, test.
|
|
|||
|
Allot of things can effect the IR temp meters. Angle pointed, distance, perhaps even color of part and reflection for readings. Also if battery is low you will get a false reading allot.
I have noticed a correct reading NOT using the red laser, and a far too low reading after I turned on the Laser, replaced the battery and all was fine again either way. Same thing with the display back light using it at night and the battery a bit low. I like my IR thermometer for many things, but it takes playing with sometimes to be sure a reading is the highest or correct. Basically I figure not much reason for a reading to ever be too high, but lots of reasons for it to be too low, so I check allot of ways like various angles and distances. Usually I trust the highest reading, and certainly if it's close to some other reading like a real thermometer or one of those shelf type oven thermometers. |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Cooking up an oven project... | dagobert | Powder Coating Questions | 33 | 06-09-2008 04:43 PM |
| Oven problem !!!!! | tavo1765 | Powder Coating Questions | 7 | 10-06-2005 06:21 PM |
| OVEN | 11111111 | Powder Coating Questions | 18 | 11-06-2004 04:16 PM |