Hi. I know a few people have asked about powder coating over gun parts in the past; but my question is, how does one powder coat over stamped serial numbers that are not very deep to begin with, to keep them visable? Will they show up anyway, or is there a "trick", such as candle wax in them, etc. that I need to do in the prep work (which so far is just glass bead blasting the frame and polishing the bluing off with black on a sisal)? Thanks, Jay.
|
|
|||
|
As an added note candle wax is a waste of time for powdering. 99% of the waxes on the market melt below 200F and some have a flash point below 400F, so with the right wax you could have a real safety hazard.
|
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Copy Chrome rust showing through | LeeParsons | Electroplating Questions | 3 | 08-19-2005 02:14 PM |
| Rust and pitting over steering column serial numbers. | GT750 | Metal Polishing Questions | 1 | 07-09-2003 08:42 AM |