my question is is the tape caswell sells (the green tape) good enough because it is only good to 400 degrees? isnt that kinda low? is anyone using something else alittle higher temp? and yes i know this is caswell's site and they dont like poeple promoting other products but i just think this is low and i need to know if i should order this tape when i order my plugs from caswell... thanks for any info ... randy
|
|
|||
|
Order it. I have been using it for 2 years and it does the job. Even if you go above 400 it doesn't matter, the tape has done it's job and will just harden a little and maybe curl a bit. By the time that happens it won't matter, the powder will have flowed out and mostly cured.
|
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| hi temp tape shrinking | craigcraig | Powder Coating Questions | 10 | 11-27-2004 11:04 PM |
| High Temp Powder?? | trsick | Powder Coating Questions | 13 | 10-11-2004 08:25 PM |
| high temp sheeting | craigcraig | Powder Coating Questions | 1 | 08-09-2004 12:15 AM |
| any experience w/ high temp on headers | RossL | Powder Coating Questions | 2 | 05-05-2004 08:11 PM |
| Can I use VHT high Temp with Krylon High temp radiator paint | magnus | Other Metal Finishing Questions | 1 | 05-03-2003 11:20 AM |