Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum  

Go Back   Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum > Powder Coating Questions

Notices

Powder Coating Questions Discussion Board For powder coating questions.

FREE POWDER COATING SYSTEM

Until 9/15 - Buy an HV System, Get a Regular PC System FREE! Two systems for the price of one! (Limited Time - US Customers Only)

HV Powder Coating System

Buy Now


Reply
 
Thread Tools Display Modes
  #1 (permalink)  
Old 09-22-2004, 02:48 PM
Newbie
 
Join Date: Sep 2004
Posts: 5
sportster883r
Default types of powders

Im just getting into pc'ing and was wondering if anyone can give me a link to a site that explans the different types of powders ex. epoxy, polyester etc. Im tryin to figure out what type I would use. I plan on doing a lot of automotive, atv, motorcycle parts. Any help would be great.

Thnaks
Reply With Quote
  #2 (permalink)  
Old 09-22-2004, 09:44 PM
customandsound
Guest
 
Posts: n/a
Default

http://www.caswellplating.com
Reply With Quote
  #3 (permalink)  
Old 09-26-2004, 07:46 PM
Amateur Metal Finisher
 
Join Date: Jun 2004
Location: massachusetts
Posts: 63
randygrapes218
Default

http://www.coatings.de/pcmanual.cfm this is a good book
Reply With Quote
  #4 (permalink)  
Old 11-20-2004, 09:57 PM
Newbie
 
Join Date: Nov 2004
Posts: 3
dirtbiker360
Default

Hey Sport,

Just had my motorcycle frame powder coated and I inquired about what type of powder he used on my frame. He told me he used a TGIC powder coat on the frame. He also said TGIC works well because of the resistence chemicals, UV, and has a low VOC(for some virtually none) apon curing. Just thought you might want to know.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
MIXING POWDERS turch Powder Coating Questions 7 12-01-2004 10:00 PM
Types of Alloys? scocklin Anodizing Questions 2 11-21-2004 09:33 PM
which powders ? duke Powder Coating Questions 1 09-27-2003 02:22 PM
Types of material that can be powder coated. bryaneh Powder Coating Questions 1 03-03-2003 07:31 PM
powder types DALE Powder Coating Questions 4 01-29-2003 09:32 PM


All times are GMT -4. The time now is 12:56 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.