Hi All,
I just bought and put together a cabinet sand blaster and was
wondering what you guy's are using for blasting? Glass bead,
aluminul oxcide or what.
Thank,
Art
Reply With Quote
  #2 (permalink)  
Old 10-07-2004, 04:22 PM
Newbie
 
Join Date: Jan 2004
Posts: 7
rkolpack
Default

Aluminum Oxide, 80 grit @ 90 PSI
Dick
Reply With Quote
  #3 (permalink)  
Old 10-07-2004, 04:33 PM
Experienced Metal Finisher
 
Join Date: Apr 2004
Posts: 466
jtagger19 is on a distinguished road
Default

glass beads for powdercoating
aluminum oxide or steelshoot for ceramic coatings
most people use SLAG (AKA. black beauty)cuz is very inexpencive
Reply With Quote
  #4 (permalink)  
Old 10-07-2004, 09:34 PM
customandsound
Guest
 
Posts: n/a
Default

glassbead at 60psi
ceramic i use sand at 80psi ( not good for you )
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Media Blasting BigDog Electroplating Questions 5 02-06-2005 11:25 AM
Question about media blasting. berad001 Metal Polishing Questions 1 02-04-2005 11:29 PM
Media blasting?? trsick Powder Coating Questions 4 02-02-2005 10:03 AM
Cleaning Oxidized Aluminum With Sand Blasting Media? freematt Other Metal Finishing Questions 2 02-23-2004 02:22 AM
Best Blasting Media process for polishing? tomg552001 Metal Polishing Questions 5 12-23-2002 02:22 PM


All times are GMT -4. The time now is 08:47 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.