Forgot the link to the pictures.
http://f1.pg.photos.yahoo.com/ph/flo...85&.src=ph

It started as a pizza oven. I bought it off Ebay for $60.00. The walls used to be sections from a roll up steel garage door. They are 2" thick and 2' wide. I stacked 2 sections on top of each other and welded them together. Then I packed it full of insulation and put sheet metal around the outside. The top sits on angle iron and isn't bolted down so I can raise or lower it depending on the size of an item I'm doing. The steel cabinet is my spray booth. I bought it at a garage sale for $5.00. My son was going to toss out Britney so I put her out in the shop to keep me company
Don
Reply With Quote
  #22 (permalink)  
Old 11-06-2004, 10:27 PM
Newbie
 
Join Date: Nov 2004
Posts: 5
bar_acres
Default Hey Blindumpire...

Where's your oven pictures? The link to yahoo pictures is no good.
Reply With Quote
  #23 (permalink)  
Old 11-08-2004, 12:06 PM
Newbie
 
Join Date: Feb 2004
Posts: 32
BlindUmpire
Default

The link worked for awhile...Yahoo must have a time limit? If anyone knows where to post them, let me know!
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
New guy question polarisbob Powder Coating Questions 6 04-18-2005 08:49 AM
Question for the guys out there with gas ovens getastro Powder Coating Questions 2 03-30-2005 07:17 PM
Powder coating ovens (small table top size) jkhcfo Powder Coating Questions 2 01-17-2004 09:50 AM
Peak voltage question mudwhump Anodizing Questions 6 01-14-2004 10:53 PM
Brand Newbie Aluminum Polishing Question gdsegel Metal Polishing Questions 1 04-25-2003 08:04 AM


All times are GMT -4. The time now is 12:28 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.