Old 11-10-2004, 09:38 AM
Newbie
 
Join Date: Nov 2004
Posts: 4
lato
Default Help

I am a novice at powder coating. I just bought a small powder coating system from Caswell. Also I bought black polyester powder. I sandblasted my first few pieces and coated them. Cured for 20 Min at 375 degrees. Pulled them out and let cool. Coating does not seem tough--they scratch easily. Am I doing something wrong? Do I need to use different type of powder? Is there some product for filling in rust pits on older material?
Thanks
Jamey
Reply With Quote
  #2 (permalink)  
Old 11-10-2004, 12:33 PM
Experienced Metal Finisher
 
Join Date: Jun 2004
Posts: 368
Popeye is an unknown quantity at this point
Default Re: Help

Lato,
Sounds like the powder is under cured. You want the BMT base metal temp at 375 before you start timing.
Caswell has Lab-Metal, works great for filling defects.
IMHO
Reply With Quote
  #3 (permalink)  
Old 11-11-2004, 12:25 AM
Experienced Metal Finisher
 
Join Date: Dec 2002
Location: Central New York
Posts: 353
DALE will become famous soon enough
Default

Is it scratching through the coating or just marring the finish?
Reply With Quote
  #4 (permalink)  
Old 11-11-2004, 12:09 PM
Newbie
 
Join Date: Nov 2004
Posts: 4
lato
Default

it is scratching all the way through to the metal, thanks jamey
Reply With Quote
  #5 (permalink)  
Old 11-11-2004, 12:10 PM
Newbie
 
Join Date: Nov 2004
Posts: 4
lato
Default

it is scratching all the way through to the metal, thanks jamey
Reply With Quote
  #6 (permalink)  
Old 11-11-2004, 09:26 PM
Amateur Metal Finisher
 
Join Date: Jan 2004
Location: Beaufort, SC
Posts: 121
WAORacing
Default

Then the part is under cured. Try setting the oven on 400 and cure for 30 min. The best and safest way is to use a infared temp gun for getting accurate temps on the part.
Reply With Quote
  #7 (permalink)  
Old 11-11-2004, 10:41 PM
Amateur Metal Finisher
 
Join Date: Oct 2004
Location: Lake Mary, FL
Posts: 56
jagboy69
Default

What is this Lab metal stuff Your telling me I can fill my cleaned metal where there are rust pits and get it smooth looking?? No way!!?? that would be awesome.. wHO has used this stuff Please tell :P
Reply With Quote
  #8 (permalink)  
Old 11-12-2004, 01:07 AM
Amateur Metal Finisher
 
Join Date: Feb 2004
Posts: 109
dagobert
Default

I've got some of it, and have been happy with the results so far. It's not for structural repairs, but for filling pits, I think you'll like it.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


All times are GMT -4. The time now is 09:14 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.