| Notices |
| Powder Coating Questions Discussion Board For powder coating questions. |
![]() |
|
|
Thread Tools | Display Modes |
|
||||
|
Ok since I have to re-strip this frame I've desided to use heat plus this will help remove the problem also. So 500 degrees for 1hr? 3 hrs?
Dale again thanks for the help...
__________________
Jim Shuster www.backyardpowdercoating.com Sold..... www.chrissys68mustang.com Hobbie www.photogserver.net Web Hosting. |
|
||||
|
Dale thanks for the reply, I'm out of here for 6 Days
I'll post a link of the Recoated frame when I get it done ... Just think only 15 more to go.... lol.. Later
__________________
Jim Shuster www.backyardpowdercoating.com Sold..... www.chrissys68mustang.com Hobbie www.photogserver.net Web Hosting. |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Oven temp vs part temp | getastro | Powder Coating Questions | 4 | 10-01-2007 12:53 AM |
| Emissivity setting for IR temp. | LouisT | Powder Coating Questions | 0 | 05-16-2005 12:04 AM |
| High Temp Powder?? | trsick | Powder Coating Questions | 13 | 10-11-2004 08:25 PM |
| IR Temp Probes | getastro | Powder Coating Questions | 3 | 07-21-2004 09:12 AM |
| Can I use VHT high Temp with Krylon High temp radiator paint | magnus | Other Metal Finishing Questions | 1 | 05-03-2003 11:20 AM |