Default pre bake and metal discoloration

When I prebake parts, such as an air cleaner, to outgas it and burn the oil out of the seams they always darken to a blue color. I realize that the metal is OK when this happens but it is necessary to resandblast the part to remove the discolorization or can the part just be coated as is? I have been resandblasting but it seems like I am doing the same thing twice here.
Reply With Quote
  #2 (permalink)  
Old 11-24-2004, 04:03 PM
Noob2PC's Avatar
Experienced Metal Finisher
 
Join Date: Mar 2004
Location: Greensboro NC
Posts: 315
Noob2PC
Default

I have never blasted Steel or Tim after prebaking. I have never had mine turn blue either.

Are you from PFF?
Reply With Quote
  #3 (permalink)  
Old 11-24-2004, 07:05 PM
Experienced Metal Finisher
 
Join Date: Apr 2004
Posts: 466
jtagger19 is on a distinguished road
Default

this happens to me with some valve covers
I always re-blast them , better sure than sorry .
Reply With Quote
  #4 (permalink)  
Old 11-24-2004, 11:51 PM
Newbie
 
Join Date: Nov 2004
Posts: 26
Electrathon
Default

Quote:
Originally Posted by Noob2PC
I have never blasted Steel or Tim after prebaking. I have never had mine turn blue either.

Are you from PFF?
Yes, Electrathon there too.

It is amazing how small the world can be. two fiero people migrating here.
Reply With Quote
  #5 (permalink)  
Old 11-25-2004, 11:09 PM
customandsound
Guest
 
Posts: n/a
Default

i have had parts discolor when preheating i shot them with no problems at all
Reply With Quote
  #6 (permalink)  
Old 11-26-2004, 12:51 PM
Noob2PC's Avatar
Experienced Metal Finisher
 
Join Date: Mar 2004
Location: Greensboro NC
Posts: 315
Noob2PC
Default

Quote:
Originally Posted by Electrathon
Quote:
Originally Posted by Noob2PC
I have never blasted Steel or Tim after prebaking. I have never had mine turn blue either.

Are you from PFF?
Yes, Electrathon there too.

It is amazing how small the world can be. two fiero people migrating here.
We also need to get together and discuse pricing. There is not Way I can price things as low as you are doing. I think we could both benefit on PFF if we both have similar pricing. Shot me a PM on PFF with your email and I will send you my pricing. Yes I am getting the prices on the sheet, we need to stand up and tell them cheapskates TDB! Yopu are selling stuff way too cheap for the work that goes into it.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


All times are GMT -4. The time now is 03:13 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.