Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum  

Go Back   Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum > Powder Coating Questions

Notices

Powder Coating Questions Discussion Board For powder coating questions.

FREE POWDER COATING SYSTEM

Until 9/15 - Buy an HV System, Get a Regular PC System FREE! Two systems for the price of one! (Limited Time - US Customers Only)

HV Powder Coating System

Buy Now


Reply
 
Thread Tools Display Modes
  #1 (permalink)  
Old 12-13-2004, 03:34 PM
Amateur Metal Finisher
 
Join Date: Nov 2004
Posts: 95
Zpider
Default Looking for this color...

Anyone know a color as close tothis as possible?

http://store1.yimg.com/I/hopup1_1821_107201220
__________________
WEIRD Performance & Coatings
Sweden
Reply With Quote
  #2 (permalink)  
Old 12-14-2004, 02:49 PM
wso wso is offline
Newbie
 
Join Date: Sep 2004
Posts: 3
wso
Default

Looks very familiar to chrome smoke to me
Reply With Quote
  #3 (permalink)  
Old 12-15-2004, 05:48 AM
Blademan's Avatar
Experienced Metal Finisher
 
Join Date: Mar 2004
Location: Gold Beach, Oregon
Posts: 322
Blademan is on a distinguished road
Default

im pretty sure I saw a color sim to that in tiger dry book, when I get to the shop this morning I will try and find the number for you...with tiger you will have to buy 5pound min and they tend to be on the spendy side...
__________________
Pro-Tech Powder Coating
93976 Ocean Way
541-247-8168
protech@harborside.com
Gold Beach,Oregon
Reply With Quote
  #4 (permalink)  
Old 12-15-2004, 05:57 AM
Amateur Metal Finisher
 
Join Date: Nov 2004
Posts: 95
Zpider
Default

Quote:
Originally Posted by Blademan
im pretty sure I saw a color sim to that in tiger dry book, when I get to the shop this morning I will try and find the number for you...with tiger you will have to buy 5pound min and they tend to be on the spendy side...
Thanks, since i live in Sweden i think ill have to fund another supplier here, but information on the color would be helpful.
__________________
WEIRD Performance & Coatings
Sweden
Reply With Quote
  #5 (permalink)  
Old 12-15-2004, 07:54 AM
Blademan's Avatar
Experienced Metal Finisher
 
Join Date: Mar 2004
Location: Gold Beach, Oregon
Posts: 322
Blademan is on a distinguished road
Default

went thru all my color charts, even looked at the wheel in adobe photo shop and to be honest its really hard to tell for sure the actual color, it appears to be two different colors depending on which monitor im useing, but my guess is looking at some things ive shot with black chrome is its black chrome, now im on a quest..going to go down to the tire shop and grab a bunch of there rim charts to see if i can find out for sure..all n all I think the black chrome will be real close..
__________________
Pro-Tech Powder Coating
93976 Ocean Way
541-247-8168
protech@harborside.com
Gold Beach,Oregon
Reply With Quote
  #6 (permalink)  
Old 12-15-2004, 07:59 AM
Amateur Metal Finisher
 
Join Date: Nov 2004
Posts: 95
Zpider
Default

Looked at Caswells limited gold, seems close but hard to determine by their webpage, anyone got any image of something coated with Limited Gold?
__________________
WEIRD Performance & Coatings
Sweden
Reply With Quote
  #7 (permalink)  
Old 12-17-2004, 07:48 PM
warchild's Avatar
Amateur Metal Finisher
 
Join Date: Feb 2003
Location: Seymour,Tn.
Posts: 147
warchild
Default

I used chrome smoke and it does look like that.
__________________
WARCHILD
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
looking for a certian color poconochoppers Powder Coating Questions 0 09-14-2004 01:08 PM
Color depth vs. anodizing time NeoMoses Anodizing Questions 17 02-03-2004 09:06 PM
Trouble getting Sand Blasted Aluminum to take color. LogicPB Anodizing Questions 7 06-05-2003 04:42 AM
color fade anno krazi_ivan Anodizing Questions 0 04-13-2003 11:40 PM
Anodizing not holding color slug Electroplating Questions 1 03-17-2003 05:46 PM


All times are GMT -4. The time now is 06:12 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.