Does or have anyone done this yet? If so doe you cure the first coat or do you spray the first coat then change to the second coat and after both coats have been applied then you put in the oven to cure? Please let me know.
Thanks, Hangman15 |
|
||||
|
Ive used the pre mixed and then i bought a 1/2 once of the powder and mixed it in with several different powders ,both came out awesome...I havent mixed in with a clear coat though.one thing though its a real pain in the butt to clean up after using anything with the illusion in it, its so fine.
__________________
Pro-Tech Powder Coating 93976 Ocean Way 541-247-8168 protech@harborside.com Gold Beach,Oregon |
|
|||
|
I always mix mine into the clearcoat.It gives you a colored metallic suspended in the clear.Very cool looking.I bake first coat and then apply and bake second coat. It is a pain to clean out of the gun. I clean the gun then when spraying next color I let the gun blow into the booth for a min to help get anything out that I may have missed. The effects of this powder can be varied by simply adjusting the mix ratio and if you shoot it straight onto a base color expect the part to appear a slightly different color.
|
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| *** WE ARE GIVING AWAY FREE POWDER COATING *** | mcaswell | Powder Coating Questions | 197 | 07-08-2008 01:31 PM |
| powder coating over powder coat? | corybarta | Powder Coating Questions | 6 | 08-21-2006 09:15 AM |
| Powder coating on firearms | LoneGunman | Powder Coating Questions | 2 | 06-15-2006 01:54 PM |
| New Product - Illusions Powder Coating | mcaswell | Powder Coating Questions | 1 | 03-11-2004 06:06 PM |
| Non-paint powder coating | dshepherd | Powder Coating Questions | 6 | 01-26-2004 12:49 PM |