Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum  

Go Back   Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum > Powder Coating Questions

Notices

Powder Coating Questions Discussion Board For powder coating questions.

Reply
 
Thread Tools Display Modes
  #131 (permalink)  
Old 03-05-2006, 04:06 PM
chromeitout's Avatar
Amateur Metal Finisher
 
Join Date: Feb 2006
Location: Pickens, SC
Posts: 143
chromeitout is an unknown quantity at this point
Default Re: *** WE ARE GIVING AWAY FREE POWDER COATING ***

I tried to post a picture of Glossy Silver on a bracket from my '90 300ZX TT but I don't think it worked. I e-mailed it to web***@caswellplating.com. I'm not exactly an internet guru so if I didn't do it right either let me know. If accepted I would like a pound of Artic Ice.

Last edited by lcaswell; 03-05-2006 at 10:24 PM.
Reply With Quote
  #132 (permalink)  
Old 03-05-2006, 05:28 PM
BigDog's Avatar
Amateur Metal Finisher
 
Join Date: Dec 2004
Posts: 89
BigDog is on a distinguished road
Default Re: *** WE ARE GIVING AWAY FREE POWDER COATING ***

Quote:
Originally Posted by chromeitout
I tried to post a picture of Glossy Silver on a bracket from my '90 300ZX TT but I don't think it worked. I e-mailed it to web***@caswellplating.com. I'm not exactly an internet guru so if I didn't do it right either let me know. If accepted I would like a pound of Artic Ice.
If you want to send me a copy of the pic i would be glad to post it for you jeffb1135@yahoo.com
__________________
Jeff B.
Instructions for riding a Warrior: 1) sit on bike, 2) start bike and idle till warm, 3) pull in clutch and put in gear, 4) release clutch and rip on the throttle, 5) {VERY IMPORTANT!!} HOLD THE F*** ON!!!, 6) Enjoy!! Side effects may include whiplash, wrinkle free skin, and an evil smile resembling the "Joker".

Last edited by lcaswell; 03-05-2006 at 10:25 PM.
Reply With Quote
  #133 (permalink)  
Old 03-05-2006, 11:17 PM
chromeitout's Avatar
Amateur Metal Finisher
 
Join Date: Feb 2006
Location: Pickens, SC
Posts: 143
chromeitout is an unknown quantity at this point
Default Re: *** WE ARE GIVING AWAY FREE POWDER COATING ***

Thanks Big Dog, I just e-mailed it to you.
Reply With Quote
  #134 (permalink)  
Old 03-08-2006, 06:37 PM
chromeitout's Avatar
Amateur Metal Finisher
 
Join Date: Feb 2006
Location: Pickens, SC
Posts: 143
chromeitout is an unknown quantity at this point
Default Re: *** WE ARE GIVING AWAY FREE POWDER COATING ***

Thanks for posting the picture Big Dog. I don't know what I'm doing wrong. Maybe someone will explain it to me. Atleast I see it worked for you.
Reply With Quote
  #135 (permalink)  
Old 03-13-2006, 03:47 PM
Newbie
 
Join Date: Jun 2005
Posts: 22
touchetj69
Default Re: *** WE ARE GIVING AWAY FREE POWDER COATING ***

We have pics in colors you do not have pics of one is Emerald and the other is Xtreme Chrome w/ Prism Additive. Not sure what color we could get for Xtreme Chrome w/ Prism Additive. Just let us know if you can use it. If you use our pics of Emerald could we please get a lb. of Candy Apple Thank You. The Pics. are in our Album key word Emerald, & Xtreme Chrome w/Prism.
Attached Thumbnails
we-giving-away-free-powder-coating-emerald-green0002.jpg   we-giving-away-free-powder-coating-img_0047.jpg  
Reply With Quote
  #136 (permalink)  
Old 03-14-2006, 02:15 PM
lcaswell's Avatar
Caswell Inc President
 
Join Date: Jan 2001
Location: Lyons NY USA
Posts: 2,366
Blog Entries: 3
lcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud of
Default Re: *** WE ARE GIVING AWAY FREE POWDER COATING ***

Thanks for the pics. Shipping free powder today.
__________________
--
Lance Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm

Please support the moderators on our site by leaving reputation for their helpful posts. Read more here.
Reply With Quote
  #137 (permalink)  
Old 03-27-2006, 07:11 PM
Newbie
 
Join Date: Nov 2005
Location: Merchantville NJ
Posts: 14
BLOWNTRC5 is on a distinguished road
Default Re: *** WE ARE GIVING AWAY FREE POWDER COATING ***

Here's a few pics of Candy Raspberry over Silver Sparkle Metallic. If used I would like a lb. of Lolypop blue.

Thanks,
Doug
Attached Thumbnails
we-giving-away-free-powder-coating-ras1.jpg   we-giving-away-free-powder-coating-ras2.jpg  
Reply With Quote
  #138 (permalink)  
Old 03-30-2006, 11:42 AM
Amateur Metal Finisher
 
Join Date: Mar 2005
Posts: 108
wamontgomery
Default Re: *** WE ARE GIVING AWAY FREE POWDER COATING ***

Quote:
Originally Posted by BLOWNTRC5
Here's a few pics of Candy Raspberry over Silver Sparkle Metallic. If used I would like a lb. of Lolypop blue.

Thanks,
Doug
Wow, that's very cool looking!
Reply With Quote
  #139 (permalink)  
Old 03-30-2006, 12:20 PM
Newbie
 
Join Date: Nov 2005
Location: Merchantville NJ
Posts: 14
BLOWNTRC5 is on a distinguished road
Default Re: *** WE ARE GIVING AWAY FREE POWDER COATING ***

Thanks,
My customer fliped over the color, he just droped off a buch of other parts for his boat to be done in the same color. Looks like I'll be ordering about another 5lbs. very soon!!!!

Doug
Reply With Quote
  #140 (permalink)  
Old 03-31-2006, 09:21 AM
Newbie
 
Join Date: Jan 2006
Posts: 2
scott61663 is on a distinguished road
Default Re: *** WE ARE GIVING AWAY FREE POWDER COATING ***

mike here is a pic of an ignition cover off of my 520 KTM done in bay mist. If my pic qualifies as being the first done in bay mist i would like to request a pound of candy apple. the url is bay mist. thanks scott
Attached Thumbnails
we-giving-away-free-powder-coating-bay-mist.jpg  
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
powder coating over powder coat? corybarta Powder Coating Questions 6 08-21-2006 09:15 AM
Powder coating on firearms LoneGunman Powder Coating Questions 2 06-15-2006 01:54 PM
New to powder coating ? customandsound Powder Coating Questions 0 06-21-2005 03:00 AM
Non-paint powder coating dshepherd Powder Coating Questions 6 01-26-2004 12:49 PM
Powder coating process.. tomg552001 Powder Coating Questions 4 01-14-2003 08:42 PM


All times are GMT -4. The time now is 09:07 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.