Old 06-14-2005, 12:38 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,358
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

Ok - these colors were accepted. Thanks.

seanc:Safety Orange:Black Magic
HardcoreZ28:Mayan Gold:Red
johnny933:Green Sparkle:Sandy Tan

I fixed the Chameleon link.

Yes, hotwheels would be ok, as long as the color is nice and clear, and truly representative of the color.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
  #72 (permalink)  
Old 06-14-2005, 08:59 PM
Newbie
 
Join Date: Dec 2004
Location: mn
Posts: 48
clydes is an unknown quantity at this point
Default psycho yellow alternator bracket for a small block chevy

altenator bracket for a chevy small block. if selected a pound of tropic orange would be great. pic is in the album

http://www.caswellplating.com/bbs/al...php?pic_id=566
Reply With Quote
  #73 (permalink)  
Old 06-14-2005, 09:51 PM
Zinc Plating Guru
 
Join Date: Jun 2003
Posts: 321
seanc is on a distinguished road
Default

Quote:
these colors were accepted. Thanks.

seanc:Safety Orange:Black Magic
Caswell, thanks! I was beginning to wonder if this offer had faded away.

I'll order some more colors to try out.
Reply With Quote
  #74 (permalink)  
Old 06-15-2005, 02:04 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,358
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

Clydes:

Any change of a bigger, clearer picture? It's a bit fuzzy.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
  #75 (permalink)  
Old 06-15-2005, 02:16 PM
Newbie
 
Join Date: Dec 2004
Location: mn
Posts: 48
clydes is an unknown quantity at this point
Default psycho yellow alternator bracket for a small block chevy

hope that helps its in the albums,tks clydes
Reply With Quote
  #76 (permalink)  
Old 06-15-2005, 02:50 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,358
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

Yep. Better. We'll use that one.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
  #77 (permalink)  
Old 06-29-2005, 09:15 AM
Amateur Metal Finisher
 
Join Date: Mar 2005
Posts: 202
mtnbiker is an unknown quantity at this point
Default Yellow and Wrinkle black

"Yellow"
http://www.caswellplating.com/bbs/al...php?pic_id=572

"Wrinkle Black"
http://www.caswellplating.com/bbs/al...php?pic_id=571

"Black Cat"
http://www.caswellplating.com/bbs/al...php?pic_id=574

Can I tell you the 3 powders I want with my next order? It is coming very soon.
Thanks
Ken H.
Reply With Quote
  #78 (permalink)  
Old 07-20-2005, 10:51 PM
Amateur Metal Finisher
 
Join Date: Jun 2005
Posts: 51
crazy_mtb_2002
Default

Hey, here's a lollypop red job i did on a bike rotor,
http://www.caswellplating.com/bbs/al...php?pic_id=578
if selected could you please send me a pound of lollypop blue? thanks alot!

By the way this powder is so nice, the angle shown is alright, but it does'nt bring out it's shinyness, in the sun the red just reflects everywhere, it's very smooth, and overall it impressed me, thanks.

PS, i am wanting to order some powder soon, so it would be easier just to throw the lollypop blue in with the order, i live in canada, and i deal with caswell canada, is it possible to just get the free powder from them, instead of shipping over the boarder? thanks alot.
Reply With Quote
  #79 (permalink)  
Old 07-26-2005, 09:41 AM
Newbie
 
Join Date: Feb 2004
Posts: 1
Neptaone
Default Post subject: *** WE ARE GIVING AWAY FREE POWDER COATING ***

Ford 8inch Rear end

Pic 1 Ford Center Section:
PCP4043 Netallic Brushed Nickel
http://www.caswellplating.com/bbs/al...php?pic_id=581

Pic 2 Ford Rear end
Center Section PCP4043 Netallic Brushed Nickel
Rearend Housing PCP51008
http://www.caswellplating.com/bbs/al...php?pic_id=580
Reply With Quote
  #80 (permalink)  
Old 08-22-2005, 10:00 PM
Zinc Plating Guru
 
Join Date: Jun 2003
Posts: 321
seanc is on a distinguished road
Default Re: *** WE ARE GIVING AWAY FREE POWDER COATING ***

I hope this offer is still going. Here's samples of Dodger Blue

http://forum.caswellplating.com/phot...o.php?photo=37

http://forum.caswellplating.com/phot...o.php?photo=38

If accepted, I'd like a can of US Blue

Thanks
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
powder coating over powder coat? corybarta Powder Coating Questions 6 08-21-2006 09:15 AM
Powder coating on firearms LoneGunman Powder Coating Questions 2 06-15-2006 01:54 PM
New to powder coating ? customandsound Powder Coating Questions 0 06-21-2005 03:00 AM
Non-paint powder coating dshepherd Powder Coating Questions 6 01-26-2004 12:49 PM
Powder coating process.. tomg552001 Powder Coating Questions 4 01-14-2003 08:42 PM


All times are GMT -4. The time now is 08:55 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.