    Want free powder, here's how:

    1. Check the pages below to see which colors we need. Any color chips that say "Photo of Actual Part" under them, we DON'T NEED.
    - http://www.caswellplating.com/powder/powder_colors.html
    - http://www.caswellplating.com/powder...r_colors2.html

    1. Buy one of the powders we need a picture of. You must have purchased the powder from us. i.e. You can't use another company's powder for a free pound of ours, and you can't use free powder from this offer to get more free powder.

    2. Shoot and bake a real automotive, motorcycle or other real part (i.e. we don't want tiny parts that no-one can relate to)

    3. Take a picture of it, on a decent background, in decent light. Make sure it's nice and big, and a JPEG please.

    4. Post a picture of it in our album here: http://forum.caswellplating.com/phot...ry.php?cat=504

    5. Reply to this post and tell us which picture is yours, and what powder you used, and what the part is. Don't forget to include the URL to the picture in the album.

    6. Assuming the picture is good enough to use, we'll send you ONE FREE POUND of whatever color you used, or a color of equal or lesser value. Let us know which one you want. Free ground shipping on that pound too.

    There is an element of risk here, in that it's possible for you to buy a color, then someone else gets their picture up first, and we don't need it anymore. Please accept that risk if you want to play. Advice, start with the less common colors.

    If you already have posted a picture and want us to use it, or we have already used a picture of yours, let us know and we'll give you retroactive credit for a pound.

    And, of course, once posted to the album, all pictures become the exclusive property of Caswell Inc.

    Happy coating!
    Last edited by mcaswell; 11-27-2005 at 05:09 PM.
    --
    Mike Caswell
    Caswell Inc
    http://www.caswellplating.com
    Need Support? Visit our online support section at http://support.caswellplating.com
    Have A Web Site?
    Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  2. #2
    Join Date
    Mar 2004
    Location
    Greensboro NC
    Posts
    315
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  3. #3
    Join Date
    Apr 2004
    Location
    Burton, Michigan
    Posts
    108

    Default

    Corvette Rear Caliper in Orange 56006

    If accepted, can I get a pound of Mercedes Silver?

    Thanks,
    Kris

    EDIT: For URL

    http://www.caswellplating.com/bbs/al...php?pic_id=315
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  4. #4
    Join Date
    Nov 2001
    Location
    Lyons, NY USA
    Posts
    1,793

    Default

    Sorry, can you please also post the URL to your pictures in the album. Thanks
    --
    Mike Caswell
    Caswell Inc
    http://www.caswellplating.com
    Need Support? Visit our online support section at http://support.caswellplating.com
    Have A Web Site?
    Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  5. #5
    Join Date
    Feb 2004
    Location
    Hermitage, PA
    Posts
    69

    Default

    caswell,

    I guess that I will be the first to stake a claim. That is my picture of Safety Red that you are already using.

    http://caswellplating.com/bbs/album_...fc757d5ac7b495

    Thanks,

    Jim
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  6. #6
    Join Date
    Feb 2004
    Location
    Hermitage, PA
    Posts
    69

    Default

    caswell,

    Here is a header done in Caswell Hi Temp Silver.

    http://www.caswellplating.com/bbs/al...php?pic_id=316

    Jim
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  7. #7
    Join Date
    Nov 2001
    Location
    Lyons, NY USA
    Posts
    1,793

    Default Previously Posted Photos Approved

    Thanks for those. The following users will be sent the following FREE powders:

    1. noob2pc - Black Magic & Safety Yellow
    2. remotestartdepot - Mercedes Silver
    3. viper56 - Safety Red & Hi Temp Burner Black
    4. mkewl - Dark Purple

    Let me know before Monday if you want a different color.
    --
    Mike Caswell
    Caswell Inc
    http://www.caswellplating.com
    Need Support? Visit our online support section at http://support.caswellplating.com
    Have A Web Site?
    Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  8. #8
    Join Date
    Oct 2004
    Location
    Parkersburg WV
    Posts
    9

    Default Lolipop Blue

    Had the chance today to try one of my new colors which is the lolipop blue. This is a transparent color. In the three pics posted, there is no base, just bare metal after it was glass beaded. O a nieghbor kid wanted me to "try" this new color to his bike pegs.. After this now he wants his bike done the same way.. Also if Caswell likes the pics Ill gladly take another pound of lolipop blue.. of course.....

    http://www.caswellplating.com/bbs/al...php?pic_id=319
    http://www.caswellplating.com/bbs/al...php?pic_id=318
    http://www.caswellplating.com/bbs/al...php?pic_id=317
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  9. #9
    Join Date
    Nov 2001
    Location
    Lyons, NY USA
    Posts
    1,793

    Default

    Thanks, but we already have a picture of the Lollypop Blue. Please check the two webpages referenced in the first post for the colors we need.
    --
    Mike Caswell
    Caswell Inc
    http://www.caswellplating.com
    Need Support? Visit our online support section at http://support.caswellplating.com
    Have A Web Site?
    Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  10. #10
    Join Date
    Oct 2004
    Location
    Parkersburg WV
    Posts
    9

    Default Dark Purple

    Ok. I jumped off the lolipop blue and see that there are no pics of the dark purple. Enjoy.. Hope this will get me that 1lb of powder.

    http://www.caswellplating.com/bbs/al...php?pic_id=322
    http://www.caswellplating.com/bbs/al...php?pic_id=321
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

+ Reply to Thread
Page 1 of 21
1 2 3 11 ... LastLast

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

     

Similar Threads

  1. powder coating over powder coat?
    By corybarta in forum Powder Coating Questions
    Replies: 6
    Last Post: 08-21-2006, 08:15 AM
  2. Powder coating on firearms
    By LoneGunman in forum Powder Coating Questions
    Replies: 2
    Last Post: 06-15-2006, 12:54 PM
  3. New to powder coating ?
    By customandsound in forum Powder Coating Questions
    Replies: 0
    Last Post: 06-21-2005, 02:00 AM
  4. Non-paint powder coating
    By dshepherd in forum Powder Coating Questions
    Replies: 6
    Last Post: 01-26-2004, 11:49 AM
  5. Powder coating process..
    By tomg552001 in forum Powder Coating Questions
    Replies: 4
    Last Post: 01-14-2003, 07:42 PM

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts

Search Engine Friendly URLs by vBSEO 3.5.0 RC1 PL1