Default shop vac?

i am building a box type spray booth and i am going to be using a filter system like the one viper uses (it is under the spray booth topic) so i need a shop vac. my question is, is there a certain one i need to buy so it doesnt explode ir will it be all right because i an using a filter plus the shop vac filter?
Reply With Quote
  #2 (permalink)  
Old 01-07-2005, 12:20 AM
Amateur Metal Finisher
 
Join Date: Feb 2004
Location: Hermitage, PA
Posts: 69
viper56
Send a message via Yahoo to viper56
Default

randygrapes218;

The motor that I am using does not allow the dust to come in contact with the motor. Powder dust can ignite when free flowing through the air. Most people have experienced a "small" explosion when discharging the gun and the spark ignites the dust. Some people use a regular shop vac and have had no problems, but they do have explosion proof type vacuums available, but at a higher cost. That is the reason why I use an air vac when cleaning my booth, no contact with an electric motor. I have found it be safer than sorry. JMHO.

Jim
Reply With Quote
  #3 (permalink)  
Old 01-07-2005, 09:44 AM
Amateur Metal Finisher
 
Join Date: Jun 2004
Location: massachusetts
Posts: 63
randygrapes218
Default

jim i noticed the vac you had on your booth but where could i ride that? i have never seen anything like it. it looks more like a pump than a vac
Reply With Quote
  #4 (permalink)  
Old 01-07-2005, 05:10 PM
Amateur Metal Finisher
 
Join Date: Feb 2004
Location: Hermitage, PA
Posts: 69
viper56
Send a message via Yahoo to viper56
Default

randygrapes218,

It is actually just a large commercial exhaust blower motor that was attached to a large tank and was used on a hard-piped vac system in a woodshop. If you are making your booth portable, you could just use a strong shop vac and just attach it to the plumbing when the booth is in use.

Jim
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Looking for a Anodizing shop in Mass. trsick Powder Coating Questions 0 05-18-2005 11:01 AM
HOBBY SHOP PLATERS ATTENTION... etcc Electroplating Questions 0 03-29-2005 08:38 AM
My new amateur PC shop viper56 Powder Coating Questions 10 05-21-2004 01:11 PM
In a bind... a local machine shop needs some help Easttex Anodizing Questions 4 04-03-2004 02:32 AM
---SHOP SIZE--- tangnut Powder Coating Questions 1 09-21-2003 08:12 PM


All times are GMT -4. The time now is 02:46 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.