Default to strip or not to strip?

#1 Can you powder coat over exsisting powder coat without stripping off the old powder ? The new powder is a different color than the base coat. #2 If the old powder does have to be stripped first ,will steel shot damage the base metal aluminum? Thanks in advance.............John
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #2 (permalink)  
Old 01-25-2005, 04:51 AM
Blademan's Avatar
Experienced Metal Finisher
 
Join Date: Mar 2004
Location: Gold Beach, Oregon
Posts: 322
Blademan is on a distinguished road
Default

yes you can coat over the old pc but not recommended...., I would suggest you strip the item and recoat. as far as the steel shot I cant say cause Ive never used it.
__________________
Pro-Tech Powder Coating
93976 Ocean Way
541-247-8168
protech@harborside.com
Gold Beach,Oregon
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #3 (permalink)  
Old 01-25-2005, 11:21 AM
Amateur Metal Finisher
 
Join Date: Dec 2004
Location: Overland Park Ks
Posts: 89
kchotboat
Default

If you leave the old powder on I would use steel wool or 220 sand paper.
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #4 (permalink)  
Old 01-25-2005, 04:43 PM
Experienced Metal Finisher
 
Join Date: Apr 2004
Posts: 483
jtagger19 is on a distinguished road
Default

I get things steel shot at a local machine shop and haven't had any problems so far.
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
Closed Thread

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


Similar Threads
Thread Thread Starter Forum Replies Last Post
Guys, there's gotta be a better way to strip powdercoating! Heavykote Powder Coating Questions 12 07-03-2005 10:10 AM
how to strip anodizing? broker1234 Anodizing Questions 1 01-17-2005 02:35 AM
Procedure to strip anodized layer off aluminum. remarc1 Other Metal Finishing Questions 1 07-27-2004 05:41 PM
Best Way to strip Chrome Live2Ride_88 Metal Polishing Questions 9 03-16-2004 04:25 PM
Can you electro strip chrome with pickle #3? tbloss001 Electroplating Questions 3 06-06-2003 10:36 AM


All times are GMT -4. The time now is 08:18 AM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2009, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.3.0
Copyright © Caswell Inc.