Default PC'ing an entire Toyota FJ40 Body.....Help

Despite all of my efforts, I cannot find any sites where someone has at least tried to PC an entire auto body. I see where BMW is using a low cure PC clear coat, but that's it.
This is a restored 1967 off-road vehicle;
I'm not looking for a show-quality finish. Durability is more important than wax-ability.

The body is sans paint and anything other than metal.
I have plenty of plaques.
It would actually be cheaper than a 2-part urethane liquid paint.

I'm not too worried about warpage because the steel is well supported.
I have removed all of the rust and there is no filler on it.
Any filling will be done with Lab Metal.

Any links, suggestions, thoughts, money....would be appreciated.
Thanks,
Brog


Here is a link of the color that I am going for.....Mustard

Reply With Quote
  #2 (permalink)  
Old 02-21-2005, 05:34 PM
Experienced Metal Finisher
 
Join Date: Dec 2002
Location: Central New York
Posts: 353
DALE will become famous soon enough
Default

Provided you have the space and equipment to do the job then you should have no problem. If you are worried about warpage simply let it cool slowly and it shouldn't warp much if any.Several auto manufacturers have gone to powder coating as a primer.However these are virgin bodies on an automated line, heck anyone can do that.They don't have 37 years of use and abuse to deal with.

This is a massive project and I hope you get through it.I would love to see the finished project.Please keep us informed along the way so we can enjoy your progress.Oh and take lots of photos please
Reply With Quote
  #3 (permalink)  
Old 02-25-2005, 09:48 AM
Newbie
 
Join Date: Jan 2004
Posts: 5
Brog
Default

I will definitely take plenty of pictures.
Hopefully they will consist of a good looking truck and not a smoldering garage.
Thanks for the response.
Brog
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


All times are GMT -4. The time now is 08:25 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.