Hi There,
I have been approched by and engineering/fabrication shop that I do a bit of work for about protecting polished parts from scratches. I was wondering if this could be done with a Clear powder coat and i was also wondering how well would the PC stick the the polished part. These parts are going to be Mass Produced for some large chain stores and we are worryed about the parts scratching during freight/installation. so would Clear PC for polished parts work and would it affect the appearence of them much? thanks Grant |
|
|||
|
I too, have sprayed clear over polished parts, and even over fleshly zinc plated parts where I wanted to keep the luster. Also sprayed clear over an intake manifold and water pump that had been tumbled overnight.
|
|
|||
|
I have done allot of items that had been polished. I just did a dozen oval brass sailboat window frames. The customer was sick of polishing them every week only to have them oxidize again & again. The brass did darken a little when cured.
Just make sure you use a pre paint prep to clean off any old wax or polish. Good Luck Bob
__________________
www.capecodpowdercoating.com |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Clear Question? HELP!!!!!!!!!!!!! | buzzurd | Powder Coating Questions | 0 | 08-14-2004 03:12 PM |
| Problems with clear, flowout, multiple colors, more... | allcarfan | Powder Coating Questions | 3 | 08-25-2003 09:49 PM |
| Plating clear plastic | Dinosaurius | Electroplating Questions | 2 | 06-11-2003 12:06 PM |
| clear coats!!! | hue | Metal Polishing Questions | 7 | 05-08-2003 11:28 PM |
| Clear coating? | Derrick | Metal Polishing Questions | 9 | 06-16-2002 10:34 PM |