where on that site are the calipers that look like yamaha blue? i saw some calipers under powder coating but they dont show the color very well.
Reply With Quote
  #22 (permalink)  
Old 03-09-2005, 01:03 AM
Amateur Metal Finisher
 
Join Date: Feb 2005
Posts: 131
tavo1765 is an unknown quantity at this point
Default

The set by the prices down the page, its a small pic, but thats the color.
Reply With Quote
  #23 (permalink)  
Old 03-09-2005, 01:04 AM
Amateur Metal Finisher
 
Join Date: Feb 2005
Posts: 131
tavo1765 is an unknown quantity at this point
Default

How close is the lolly pop blue, what if you apply it thicker would it be close?
Reply With Quote
  #24 (permalink)  
Old 03-21-2005, 09:44 PM
Amateur Metal Finisher
 
Join Date: Feb 2005
Posts: 131
tavo1765 is an unknown quantity at this point
Default

Just got the Tiger Drylac dormant blue in today, sprayed it on a test piece and shot clear, it is the the Yamaha Blue color exact!!!

It sprays on a purple color, then cures a chrome base, then you add clear and cure, it turns the blue/purple color.
Reply With Quote
  #25 (permalink)  
Old 03-21-2005, 10:16 PM
Amateur Metal Finisher
 
Join Date: Jun 2004
Location: massachusetts
Posts: 63
randygrapes218
Default

what do you mean "then cures a chrome base"? how did it look before the the clear? and do you have any pics?
Reply With Quote
  #26 (permalink)  
Old 03-22-2005, 12:48 AM
Amateur Metal Finisher
 
Join Date: Feb 2005
Posts: 131
tavo1765 is an unknown quantity at this point
Default

You spray the purple powder on the part, cure it partially and it turns chrome is the process, now when you spray the clear on it and cure the part, it turns into the blue/purple metallic, I will do some parts tomorrow and post pics
Reply With Quote
  #27 (permalink)  
Old 04-07-2005, 02:33 AM
Amateur Metal Finisher
 
Join Date: Feb 2005
Posts: 131
tavo1765 is an unknown quantity at this point
Default

Lolly pop blue over silver and we have Yamaha Blue. Look no further because you can buy both here. Dormant is also close if not exact but the lolly over silver base is dead on.
Reply With Quote
  #28 (permalink)  
Old 04-07-2005, 09:07 PM
Amateur Metal Finisher
 
Join Date: Nov 2004
Posts: 75
corybarta is an unknown quantity at this point
Default

COOL, Can I use a metallic silver under the lolipop blue top coat or do I need a regular silver color. thanks
Reply With Quote
  #29 (permalink)  
Old 04-08-2005, 03:02 AM
Amateur Metal Finisher
 
Join Date: Feb 2005
Posts: 131
tavo1765 is an unknown quantity at this point
Default

use any kind of chrome or silver with or without flakes.

I used it over fully polished parts
Reply With Quote
  #30 (permalink)  
Old 04-09-2005, 07:49 PM
Amateur Metal Finisher
 
Join Date: Nov 2004
Posts: 75
corybarta is an unknown quantity at this point
Default

Question, when appliying the top coat do you bake the silver for about 5 minutes and then put the top coat on or do you fully cure the silver first, thanks again.
I ordered the loly pop blue also.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
candy blue, yamaha color corybarta Caswell Please Sell This... 5 03-19-2005 01:05 AM
Color depth vs. anodizing time NeoMoses Anodizing Questions 17 02-03-2004 10:06 PM
BEWARE!!! Problem Plating Car with Metallic color paint! GoldiesPlating Electroplating Questions 0 08-29-2003 10:29 PM
color fade anno krazi_ivan Anodizing Questions 0 04-14-2003 12:40 AM
Blue Anodize keith_a_bond Electroplating Questions 1 03-03-2002 08:30 PM


All times are GMT -4. The time now is 08:56 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.