    metal prep question

    I am going to powder coat some of my 4 wheeler part (racks, rims and front bumper) Do I have to sand blast all the way down to bare metal or can I just ruffen up the existing paint. Some of this factory stuff is extremely hard to blast off. Thanks guys
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  2. Join Date
    Jan 2004
    Posts
    277

    If it were me I'd take it down to the bare metal. I would also use a phosphate treatment or similar on it before I PC the parts. I know it's tough to get the old paint off but you'll end up with much better job that way. Caswells has some pretty good strippers you might think about using as well. Strip it first then blast it, and use a pretreatment to further protect the metal.
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  3. Join Date
    Dec 2004
    Location
    Overland Park Ks
    Posts
    82

    I did some headers last week and the person blasting them left a little red paint in some areas and it blead through the yellow powder now I need to redo them.
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

+ Reply to Thread

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

     

Similar Threads

  1. Prep metal for chroming
    By ggcr in forum Electroplating Questions
    Replies: 3
    Last Post: 11-26-2004, 01:27 AM
  2. Question about getting the metal up to 400 degrees...
    By Bud in forum Powder Coating Questions
    Replies: 5
    Last Post: 06-08-2004, 01:52 AM
  3. Using OSPHO for metal prep?
    By Blademan in forum Powder Coating Questions
    Replies: 0
    Last Post: 03-31-2004, 09:06 AM
  4. Lab metal question
    By NeoMoses in forum Anodizing Questions
    Replies: 6
    Last Post: 12-13-2003, 06:33 PM
  5. how to prep metal for painting
    By coorsman in forum Other Metal Finishing Questions
    Replies: 2
    Last Post: 08-16-2003, 05:26 PM

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts

Search Engine Friendly URLs by vBSEO 3.5.0 RC1 PL1